General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.08 % Show Supplier Material materials with Absorción de agua of 0.08 % | ASTM D 570 | (23°C/24hrs) |
Densidad relativa | 23.0 °C | 1.31 [-] Show Supplier Material materials with Densidad relativa of 1.31 [-] | ASTM D 792 |
Specific volume | 23.0 °C | 0.76 cm³/g Show Supplier Material materials with Specific volume of 0.76 cm³/g | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 300 % Show Supplier Material materials with Elongación of 300 % | ASTM D 638 | brk, Type I, 50 mm/min |
Gardner Impact | 23.0 °C | 40 J Show Supplier Material materials with Gardner Impact of 40 J | ASTM D 3029 | modified, 23°C |
Hardness, Rockwell R | 23.0 °C | 117 [-] Show Supplier Material materials with Hardness, Rockwell R of 117 [-] | ASTM D 785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 53 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 53 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 1602 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1602 J/m | ASTM D 4812 | 23°C |
Módulo de flexión | 23.0 °C | 2.3 GPa Show Supplier Material materials with Módulo de flexión of 2.3 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Resistencia a la flexión | 23.0 °C | 82 MPa Show Supplier Material materials with Resistencia a la flexión of 82 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Resistencia a la tracción | 23.0 °C | 51 MPa Show Supplier Material materials with Resistencia a la tracción of 51 MPa | ASTM D 638 | yld, Type I, 50 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 53 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 53 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 8.1E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 8.1E-5 1/K | ASTM E 831 | -40°C to 40°C |
Heat deflection temperature, 0.45 MPa | 154 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 154 °C | ASTM D 648 | 6.4 mm, unannealed | |
Heat deflection temperature, 1.80 MPa | 54 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 54 °C | ASTM D 648 | 6.4 mm, unannealed | |
Temperatura de flexión bajo carga | 54 - 154 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 54 - 154 °C |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Volume resistivity | 23.0 °C | 4.00E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 4.00E+16 Ω·cm | >, ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 1.5 % Show Supplier Material materials with Contracción of 1.5 % | SABIC method | 2.3-4.6 mm |
Contracción transversal | 23.0 °C | 1.6 % Show Supplier Material materials with Contracción transversal of 1.6 % | SABIC method | 2.3-4.6 mm |
Velocidad de flujo del volumen derretido | 9 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 9 cm³/10min | ISO 1133 | MVR at 250°C/2.16 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Water Treatment/Filtration, Wiring Devices, Vending Machine, Personal Care, Medical Device, Pharmaceutical Packaging & Drug Delivery, Servingware, Electronic Components, Food Processor, Heavy Vehicles, Lab Ware and Clinical Diagnostics, Air Filtration, Commercial Storage/Cookware, Wire & cable | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 110 to 120.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |