General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.35 % Show Supplier Material materials with Absorción de agua of 0.35 % | ASTM D 570 | (23°C/Saturated) |
Densidad | 23.0 °C | 1.19 g/cm³ Show Supplier Material materials with Densidad of 1.19 g/cm³ | ASTM D 792 |
Densidad relativa | 23.0 °C | 1.2 [-] Show Supplier Material materials with Densidad relativa of 1.2 [-] | ASTM D 792 |
Specific volume | 23.0 °C | 0.83 cm³/g Show Supplier Material materials with Specific volume of 0.83 cm³/g | ASTM D 792 |
Índice límite de óxigeno | 23.0 °C | 25 % Show Supplier Material materials with Índice límite de óxigeno of 25 % |
Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Dureza Rockwell M | 23.0 °C | 70 [-] Show Supplier Material materials with Dureza Rockwell M of 70 [-] | ASTM D 785 | | ||
Elongación | 23.0 °C | 70 % Show Supplier Material materials with Elongación of 70 % | ISO 527 | break, 50 mm/min | ||
Hardness, Rockwell R | 23.0 °C | 118 [-] Show Supplier Material materials with Hardness, Rockwell R of 118 [-] | ASTM D 785 | ||
Impact strength, Izod notched, ASTM | 23.0 °C | 640 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 640 J/m | ASTM D 256 | ||
Impact strength, Izod unnotched, ASTM | 23.0 °C | 3204 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 3204 J/m | ASTM D 4812 | 23°C | ||
Instrumented Impact, at Peak | 23.0 °C | 54 J Show Supplier Material materials with Instrumented Impact, at Peak of 54 J | ASTM D 3763 | 23°C | ||
Módulo de flexión | 23.0 °C | 2.3 GPa Show Supplier Material materials with Módulo de flexión of 2.3 GPa | ISO 178 | 2 mm/min | ||
Módulo elástico | 23.0 °C | 2.4 GPa Show Supplier Material materials with Módulo elástico of 2.4 GPa | ISO 527 | 1 mm/min | ||
Resistencia a la flexión | 23.0 °C | 90 MPa Show Supplier Material materials with Resistencia a la flexión of 90 MPa | ISO 178 | yield, 2 mm/min | ||
Resistencia a la tracción | 23.0 °C | 50 MPa Show Supplier Material materials with Resistencia a la tracción of 50 MPa | ISO 527 | break, 50 mm/min | ||
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 12 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 12 kJ/m² | ISO 179/1eA | V-notch Edgew, 23°C, 80*10*4 sp=62mm | ||
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 12 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 12 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C | ||
Taber Abrasion | 23.0 °C | 10 mg/1000cy Show Supplier Material materials with Taber Abrasion of 10 mg/1000cy | ASTM D 1044 | CS-17, 1 kg | ||
Resistencia al choque, ensayo Izod no entallado | ISO 180/1U | unnotched 80*10*4, -30°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball Pressure Test | nan | IEC 60695-10-2 | 125°C +/- 2°C | |||
Calor específico | 23.0 °C | 1.25E-3 J/(kg·K) Show Supplier Material materials with Calor específico of 1.25E-3 J/(kg·K) | ASTM C 351 | ||
Coeficiente de dilatación térmica | 23.0 °C | 7E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Conductividad térmica | 23.0 °C | 0.2 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.2 W/(m·K) | ISO 8302 | ||
Heat deflection temperature, 0.45 MPa | 133 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 133 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |||
Heat deflection temperature, 1.80 MPa | 121 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 121 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |||
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | UL 746B | |||
Relative temperature index, mechanical impact | 130 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 130 °C | UL 746B | |||
Relative temperature index, mechanical strength | 130 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C | UL 746B | |||
Temperatura de flexión bajo carga | 121 - 133 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 121 - 133 °C | ||||
Temperatura de reblandecimiento Vicat | 145 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 145 °C | ISO 306 | Rate A/50 | |||
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=103956751- - <br> UL Recognized, 94V-2 Flame Class Rating: ≥1.1mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥1.1mm UL 94 <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=103876512- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica, 1 MHz | 23.0 °C | 2.7 [-] Show Supplier Material materials with Constante dieléctrica, 1 MHz of 2.7 [-] | IEC 60250 |
Dielectric constant, 60Hz | 23.0 °C | 2.7 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 2.7 [-] | IEC 60250 | 50/60 Hz |
Dissipation factor, 1MHz | 23.0 °C | 0.01 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 0.01 [-] | IEC 60250 |
Dissipation factor, 50Hz | 23.0 °C | 1E-3 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 1E-3 [-] | IEC 60250 | 50/60 Hz |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
High Volt Arc Track Rate | 23.0 °C | 2 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 2 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 2 |
Rigidez dieléctrica | 23.0 °C | 17 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 17 kV/mm | IEC 60243-1 | in oil, 3.2 mm, |
Sheet resistivity, ROA | 23.0 °C | 1.00E+15 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+15 Ω | >, IEC 60093 |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm | >, IEC 60093 | |
Índice de seguimiento comparativo | 23.0 °C | 2 V Show Supplier Material materials with Índice de seguimiento comparativo of 2 V | UL 746A | (UL) {PLC} |
Óptico
Property | Value | Comment |
---|---|---|
Transmission | 88 % Show Supplier Material materials with Transmission of 88 % | ASTM D 1003 | 2.54 mm |
Turbidez | 1 % Show Supplier Material materials with Turbidez of 1 % | ASTM D 1003 | 2.54 mm |
Índice de refracción | 1.59 [-] Show Supplier Material materials with Índice de refracción of 1.59 [-] | ASTM D542 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 % Show Supplier Material materials with Contracción of 0.5 % | SABIC method | 3.2 mm |
Velocidad de flujo de la masa derretida | 25 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 25 g/10min | ASTM D 1238 | 300°C/1.2 kgf | |
Velocidad de flujo del volumen derretido | 23 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 23 cm³/10min | ISO 1133 | MVR at 300°C/1.2 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Enclosures | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |