LNP™ LUBRICOMP™ Compound MFL36S - Asia

Want to keep this datasheet? Save it now in your required format

Description

LNP LUBRICOMP MFL36S is a compound based on Polypropylene resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant.

Los datos sobre este material han sido proporcionados por Sabic.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValueComment

Densidad

23.0 °C

1.27 g/cm³

Show Supplier Material materials with Densidad of 1.27 g/cm³

ASTM D 792

Mecánica

PropertyTemperatureValueComment

Elongación

23.0 °C

2.9 %

Show Supplier Material materials with Elongación of 2.9 %

ASTM D 638 | break

Módulo de flexión

23.0 °C

5.9 GPa

Show Supplier Material materials with Módulo de flexión of 5.9 GPa

ASTM D 790

Módulo elástico

23.0 °C

7.6 GPa

Show Supplier Material materials with Módulo elástico of 7.6 GPa

ASTM D 638 | 50 mm/min

Resistencia a la flexión

23.0 °C

117 MPa

Show Supplier Material materials with Resistencia a la flexión of 117 MPa

ASTM D 790

Resistencia a la tracción

23.0 °C

71 MPa

Show Supplier Material materials with Resistencia a la tracción of 71 MPa

ASTM D 638 | break

Resistencia al choque, ensayo Izod entallado

23.0 °C

90 kJ/m²

Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 90 kJ/m²

ASTM D 256 | notched, 23°C

Rheological Properties

PropertyTemperatureValueComment

Contracción

23.0 °C

0.4 %

Show Supplier Material materials with Contracción of 0.4 %

ASTM D 955 | 24 hrs

Technological properties

Property
Application areas

Industrial Material Handling, Engine Component, Engine Cooling System, Electronic Components, Enclosures, Enclosure/Housing/Cover, Cooking Range, Auto Aftermarket, Non-LED Lighting

Availability

Europe,Asia,Americas

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.