General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.13 % Show Supplier Material materials with Absorción de agua of 0.13 % | ISO 62-1 | (23°C/saturated) |
Densidad | 23.0 °C | 1.2 g/cm³ Show Supplier Material materials with Densidad of 1.2 g/cm³ | ISO 1183 |
Densidad relativa | 23.0 °C | 1.19 [-] Show Supplier Material materials with Densidad relativa of 1.19 [-] | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.11 % Show Supplier Material materials with Moisture absorption of 0.11 % | ISO 62 | (23°C / 50% RH) |
Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Elongación | 23.0 °C | 73 % Show Supplier Material materials with Elongación of 73 % | ISO 527 | break, 50 mm/min | ||
Hardness, Ball Indentation | 23.0 °C | 138 MPa Show Supplier Material materials with Hardness, Ball Indentation of 138 MPa | ISO 2039-1 | H358/30 | ||
Impact strength, Izod notched, ASTM | 23.0 °C | 100 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 100 J/m | ASTM D 256 | ||
Instrumented Impact, Total Energy | 23.0 °C | 65 J Show Supplier Material materials with Instrumented Impact, Total Energy of 65 J | ASTM D 3763 | 23°C | ||
Módulo de flexión | 23.0 °C | 2.4 GPa Show Supplier Material materials with Módulo de flexión of 2.4 GPa | ISO 178 | 2 mm/min | ||
Módulo elástico | 23.0 °C | 2.3 GPa Show Supplier Material materials with Módulo elástico of 2.3 GPa | ISO 527 | 1 mm/min | ||
Resistencia a la flexión | 23.0 °C | 96 MPa Show Supplier Material materials with Resistencia a la flexión of 96 MPa | ISO 178 | yield, 2 mm/min | ||
Resistencia a la tracción | 23.0 °C | 63 MPa Show Supplier Material materials with Resistencia a la tracción of 63 MPa | ISO 527 | yield, 50 mm/min | ||
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*3 sp=62mm, 23°C | ||
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 10 kJ/m² | ISO 180/1A | 80*10*3, 23°C | ||
Impact strength, Izod unnotched, ASTM | ASTM D 4812 | 23°C | ||||
Resistencia al choque, ensayo Charpy no entallado | ISO 179/1eU | Unnotch Edgew 80*10*3 sp=62mm, -30°C | ||||
Resistencia al choque, ensayo Izod no entallado | ISO 180/1U | unnotched 80*10*3, -30°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball Pressure Test | Pass | IEC 60695-10-2 | 125°C +/- 2°C | |||
Coeficiente de dilatación térmica | 23.0 °C | 7.7E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7.7E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 8E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 8E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||||
Glow Wire Ignition Temperature | 850 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 850 °C | IEC 60695-2-13 | 3.0 mm | |||
Heat deflection temperature, 0.45 MPa | 131 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 131 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |||
Heat deflection temperature, 1.80 MPa | 121 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 121 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |||
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | UL 746B | |||
Relative temperature index, mechanical impact | 120 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 120 °C | UL 746B | |||
Relative temperature index, mechanical strength | 130 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C | UL 746B | |||
Temperatura de flexión bajo carga | 121 - 131 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 121 - 131 °C | ||||
Temperatura de reblandecimiento Vicat | 146 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 146 °C | ISO 306 | Rate A/50 | |||
Inflamabilidad | UL Recognized, 94V-2 Flame Class Rating: ≥0.4mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.4mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥1.5mm UL 94 <br> Glow Wire Ignitability Temperature, 1.5 mm: 850°C IEC 60695-2-13 <br> UV-light, water exposure/immersion: F1- UL 746C <br> Glow Wire Flammability Index, 1.5 mm: 960°C IEC 60695-2-12 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101088457- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica, 1 MHz | 23.0 °C | 2.7 [-] Show Supplier Material materials with Constante dieléctrica, 1 MHz of 2.7 [-] | IEC 62631-2-1 |
Dielectric constant, 1GHz | 23.0 °C | 2.78 [-] Show Supplier Material materials with Dielectric constant, 1GHz of 2.78 [-] | ASTM ES 7-83 | 1.1 GHz |
Dielectric constant, 60Hz | 23.0 °C | 2.4 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 2.4 [-] | IEC 62631-2-1 | 50/60 Hz |
Dissipation factor, 1GHz | 23.0 °C | 5.6E-3 [-] Show Supplier Material materials with Dissipation factor, 1GHz of 5.6E-3 [-] | ASTM ES 7-83 | |
Dissipation factor, 1MHz | 23.0 °C | 0.01 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 0.01 [-] | IEC 62631-2-1 |
Dissipation factor, 50Hz | 23.0 °C | 1E-3 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 1E-3 [-] | IEC 62631-2-1 | 50/60 Hz |
High Amp Arc Ignition | 23.0 °C | 0.4 mm Show Supplier Material materials with High Amp Arc Ignition of 0.4 mm | ≥, UL 746A | PLC 1 |
Hot-Wire Ignition | 23.0 °C | 0.4 mm Show Supplier Material materials with Hot-Wire Ignition of 0.4 mm | ≥, UL 746A | PLC 3 |
Rigidez dieléctrica | 23.0 °C | 18 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 18 kV/mm | IEC 60243-1 | in oil, 3.2 mm, |
Sheet resistivity, ROA | 23.0 °C | 1.00E+16 - 1.00E+17 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+16 - 1.00E+17 Ω | IEC 62631-3-2 |
Volume resistivity | 23.0 °C | 1.00E+16 - 1.00E+17 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+16 - 1.00E+17 Ω·cm | IEC 62631-3-1 |
Índice de seguimiento comparativo | 23.0 °C | 3 V Show Supplier Material materials with Índice de seguimiento comparativo of 3 V | UL 746A | (UL) {PLC} |
Óptico
Property | Value | Comment |
---|---|---|
Transmission | 91 % Show Supplier Material materials with Transmission of 91 % | >, ASTM D 1003 | 2.54 mm |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.55 % Show Supplier Material materials with Contracción of 0.55 % | SABIC method | 3.2 mm |
Contracción transversal | 23.0 °C | 0.6 % Show Supplier Material materials with Contracción transversal of 0.6 % | SABIC method | 3.2 mm |
Velocidad de flujo de la masa derretida | 18 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 18 g/10min | ASTM D 1238 | 300°C/1.2 kgf | |
Velocidad de flujo del volumen derretido | 17 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 17 cm³/10min | ISO 1133 | MVR at 300°C/1.2 kg |
Technological properties
Property | ||
---|---|---|
Application areas | LED Lighting, Non-LED Lighting | |
Availability | Europe,Asia,Americas | |
Processing methods | Screw Speed: 40 to 70.0rpm | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |