Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 6.2 % Show Supplier Material materials with Elongación of 6.2 % | ASTM D 638 | yld, Type I, 50 mm/min |
Módulo de flexión | 23.0 °C | 2.3 GPa Show Supplier Material materials with Módulo de flexión of 2.3 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Módulo elástico | 23.0 °C | 2.3 GPa Show Supplier Material materials with Módulo elástico of 2.3 GPa | ASTM D 638 | 50 mm/min |
Resistencia a la flexión | 23.0 °C | 93 MPa Show Supplier Material materials with Resistencia a la flexión of 93 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Resistencia a la tracción | 23.0 °C | 68 MPa Show Supplier Material materials with Resistencia a la tracción of 68 MPa | ASTM D 638 | brk, Type I, 50 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 854 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 854 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 137 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 137 °C | ASTM D 648 | 3.2 mm, unannealed | |
Heat deflection temperature, 1.80 MPa | 126 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 126 °C | ASTM D 648 | 3.2mm, unannealed | |
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | UL 746B | |
Relative temperature index, mechanical impact | 130 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 130 °C | UL 746B | |
Relative temperature index, mechanical strength | 130 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C | UL 746B | |
Temperatura de flexión bajo carga | 126 - 137 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 126 - 137 °C | ||
Inflamabilidad | UL Recognized, 94HB Flame Class Rating: ≥0.7mm UL 94 <br> UV-light, water exposure/immersion: F2- UL 746C <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=220937- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 1.14 mm Show Supplier Material materials with High Amp Arc Ignition of 1.14 mm | ≥, UL 746A | PLC 2 |
High Volt Arc Track Rate | 23.0 °C | 2 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 2 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 2 |
Índice de seguimiento comparativo | 23.0 °C | 2 V Show Supplier Material materials with Índice de seguimiento comparativo of 2 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 % Show Supplier Material materials with Contracción of 0.5 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Application areas | Wireless Communications, Wiring Devices, Sunglasses, Small Appliance, LED Lighting, Personal Computing, Non-LED Lighting, Personal Care, Enclosures, Enclosure/Housing/Cover, Electronics, Electronic Components, Game Player, Food Processor, Document Handling, Doors Hardware/Trim, Displays, Data Transfer, Data Management, Audio, Air Cabin Interiors | |
Availability | Europe,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |