General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 4.2 % Show Supplier Material materials with Absorción de agua of 4.2 % | ISO 62-1 | (23°C/saturated) |
Densidad | 23.0 °C | 1.1 g/cm³ Show Supplier Material materials with Densidad of 1.1 g/cm³ | ISO 1183 |
Densidad relativa | 23.0 °C | 1.09 [-] Show Supplier Material materials with Densidad relativa of 1.09 [-] | ASTM D 792 | |
Moisture absorption | 23.0 °C | 1.2 % Show Supplier Material materials with Moisture absorption of 1.2 % | ISO 62 | (23°C / 50% RH) |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 30 % Show Supplier Material materials with Elongación of 30 % | ISO 527 | break, 50 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 130 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 130 J/m | ASTM D 256 | notched, 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 50 J Show Supplier Material materials with Instrumented Impact, Total Energy of 50 J | ASTM D 3763 | 23°C |
Módulo de flexión | 23.0 °C | 2.3 GPa Show Supplier Material materials with Módulo de flexión of 2.3 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 2.3 GPa Show Supplier Material materials with Módulo elástico of 2.3 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 90 MPa Show Supplier Material materials with Resistencia a la flexión of 90 MPa | ISO 178 | yield, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 55 MPa Show Supplier Material materials with Resistencia a la tracción of 55 MPa | ISO 527 | break, 50 mm/min |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*4 sp=62mm, -30°C |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 15 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 15 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Ball Pressure Test | nan | IEC 60695-10-2 | 125°C +/- 2°C | |
Coeficiente de dilatación térmica | 23.0 °C | 9E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 9E-5 1/K | ISO 11359-2 | 23°C to 60°C |
Coeficiente de dilatación térmica transversal | 23.0 °C | 9E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 9E-5 1/K | ISO 11359-2 | 23°C to 60°C |
Heat deflection temperature, 0.45 MPa | 190 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 190 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |
Temperatura de flexión bajo carga | 190 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 190 °C | ||
Temperatura de reblandecimiento Vicat | 200 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 200 °C | ISO 306 | Rate B/120 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Volume resistivity | 23.0 °C | 1000 - 10000 Ω·cm Show Supplier Material materials with Volume resistivity of 1000 - 10000 Ω·cm | SABIC method |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 1.4 % Show Supplier Material materials with Contracción of 1.4 % | SABIC method | 3.2 mm |
Contracción transversal | 23.0 °C | 1.2 % Show Supplier Material materials with Contracción transversal of 1.2 % | SABIC method | 3.2 mm |
Velocidad de flujo de la masa derretida | 20 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 20 g/10min | ASTM D 1238 | 280°C/5.0 kgf | |
Velocidad de flujo del volumen derretido | 12 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 12 cm³/10min | ISO 1133 | MVR at 280°C/5.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Wheel Cover, Vertical Body Panel, Recreational Vehicle, Skid Plate, Fuel Handling, Exterior Trim, Front Grille, Furnace/Heater, Electronic Components, Enclosures, Console, Cladding, Auto Aftermarket, Building Accessory | |
Availability | Americas | |
Processing methods | Drying Temperature: 100 to 120.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |