General
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.57 - 0.99 [-] Show Supplier Material materials with Coefficient of friction of 0.57 - 0.99 [-] | ||
Coefficient of friction, kinetic | 0.57 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.57 [-] | ASTM D 3702 Modified: Instr. | |
Coefficient of friction, static | 0.99 [-] Show Supplier Material materials with Coefficient of friction, static of 0.99 [-] | ASTM D 3702 Modified: Instr. | |
Densidad | 23.0 °C | 1.44 g/cm³ Show Supplier Material materials with Densidad of 1.44 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 4.2 % Show Supplier Material materials with Elongación of 4.2 % | ISO 527 | break, 5 mm/min |
Flexural strain | 23.0 °C | 3.9 % Show Supplier Material materials with Flexural strain of 3.9 % | ISO 178 | break, 2 mm/min |
Módulo de flexión | 23.0 °C | 8.6 GPa Show Supplier Material materials with Módulo de flexión of 8.6 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 10.2 GPa Show Supplier Material materials with Módulo elástico of 10.2 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 165 MPa Show Supplier Material materials with Resistencia a la flexión of 165 MPa | ISO 178 | break, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 250 MPa Show Supplier Material materials with Resistencia a la tracción of 250 MPa | ISO 527 | break, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 14 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 14 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 98 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod no entallado of 98 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 2.4E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.4E-5 1/K | ISO 11359-2 | 23°C to 60°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 7.5E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 7.5E-5 1/K | ISO 11359-2 | 23°C to 60°C | ||
Heat deflection temperature, 0.45 MPa | 219 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 219 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 206 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 206 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | UL 746B | |||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | UL 746B | |||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | UL 746B | |||
Temperatura de flexión bajo carga | 206 - 219 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 206 - 219 °C | ||||
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=103600532- - <br> UL Recognized, 94HB Flame Class Rating: ≥1.5mm UL 94 <br> UV-light, water exposure/immersion: F1- UL 746C |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
Hot-Wire Ignition | 23.0 °C | 2.5 mm Show Supplier Material materials with Hot-Wire Ignition of 2.5 mm | ≥, UL 746A | PLC 0 |
Índice de seguimiento comparativo | 23.0 °C | 1 V Show Supplier Material materials with Índice de seguimiento comparativo of 1 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.1 % Show Supplier Material materials with Contracción of 0.1 % | SABIC method |
Technological properties
Property | ||
---|---|---|
Application areas | METAL DOWNSTREAM INDUSTRIALS | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |