General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.04 % Show Supplier Material materials with Absorción de agua of 0.04 % | ISO 62-1 | (23°C/24hrs) |
Densidad | 23.0 °C | 1.27 g/cm³ Show Supplier Material materials with Densidad of 1.27 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 3.6 % Show Supplier Material materials with Elongación of 3.6 % | ISO 527 | break, 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 140 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 140 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 700 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 700 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 21 J Show Supplier Material materials with Instrumented Impact, Total Energy of 21 J | ASTM D 3763 | 23°C |
Módulo de flexión | 23.0 °C | 4.2 GPa Show Supplier Material materials with Módulo de flexión of 4.2 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 4.4 GPa Show Supplier Material materials with Módulo elástico of 4.4 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 132 MPa Show Supplier Material materials with Resistencia a la flexión of 132 MPa | ISO 178 | break, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 82 MPa Show Supplier Material materials with Resistencia a la tracción of 82 MPa | ISO 527 | break, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 140 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 140 kJ/m² | ASTM D 256 | notched, 23°C |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 42 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod no entallado of 42 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 4E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 4E-5 1/K | ASTM E 831 | 23°C to 80°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 8.3E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 8.3E-5 1/K | ASTM E 831 | 23°C to 80°C | ||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||||
Glow Wire Ignition Temperature | 850 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 850 °C | IEC 60695-2-13 | 1.6 mm | |||
Heat deflection temperature, 0.45 MPa | 121 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 121 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 115 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 115 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |||
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |||
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |||
Temperatura de flexión bajo carga | 115 - 121 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 115 - 121 °C | ||||
Temperatura de reblandecimiento Vicat | 123 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 123 °C | ISO 306 | Rate B/50 | |||
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=103129464- - <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.6mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.5mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.5mm UL 94 <br> Glow Wire Ignitability Temperature, 1.0 mm: 850°C IEC 60695-2-13 <br> Glow Wire Flammability Index, 1.0 mm: 960°C IEC 60695-2-12 <br> Glow Wire Flammability Index, 1.6 mm: 960°C IEC 60695-2-12 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica | 23.0 °C | 3.04 [-] Show Supplier Material materials with Constante dieléctrica of 3.04 [-] | SABIC method | 1.9 GHz |
Dielectric constant, 10GHz | 23.0 °C | 3.05 [-] Show Supplier Material materials with Dielectric constant, 10GHz of 3.05 [-] | SABIC method |
Dielectric constant, 1GHz | 23.0 °C | 3.03 [-] Show Supplier Material materials with Dielectric constant, 1GHz of 3.03 [-] | SABIC method | 1.1 GHz |
Dielectric constant, 5GHz | 23.0 °C | 3.05 [-] Show Supplier Material materials with Dielectric constant, 5GHz of 3.05 [-] | SABIC method |
Dissipation factor, 1GHz | 23.0 °C | 6.4E-3 [-] Show Supplier Material materials with Dissipation factor, 1GHz of 6.4E-3 [-] | SABIC method | |
Dissipation factor, 5GHz | 23.0 °C | 6.2E-3 [-] Show Supplier Material materials with Dissipation factor, 5GHz of 6.2E-3 [-] | SABIC method |
Factor de disipación | 23.0 °C | 6.3E-3 [-] Show Supplier Material materials with Factor de disipación of 6.3E-3 [-] | SABIC method |
Sheet resistivity, ROA | 23.0 °C | 1.00E+16 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+16 Ω | >, ASTM D 257 |
Volume resistivity | 23.0 °C | 1.00E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+16 Ω·cm | >, ASTM D 257 |
Índice de seguimiento comparativo | 23.0 °C | 3 V Show Supplier Material materials with Índice de seguimiento comparativo of 3 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.3 % Show Supplier Material materials with Contracción of 0.3 % | ASTM D 955 | 24 hrs |
Contracción transversal | 23.0 °C | 0.3 % Show Supplier Material materials with Contracción transversal of 0.3 % | ASTM D 955 | 24 hrs |
Velocidad de flujo de la masa derretida | 24 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 24 g/10min | ASTM D 1238 | 300°C/2.16 kgf | |
Velocidad de flujo del volumen derretido | 11 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 11 cm³/10min | ISO 1133 | MVR at 300°C/1.2 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Enclosure/Housing/Cover | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 110°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |