General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.18 g/cm³ Show Supplier Material materials with Densidad of 1.18 g/cm³ | ASTM D 792 |
Densidad relativa | 23.0 °C | 1.18 [-] Show Supplier Material materials with Densidad relativa of 1.18 [-] | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.43 % Show Supplier Material materials with Moisture absorption of 0.43 % | ISO 62 | (23°C / 50% RH) |
Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Elongación | 23.0 °C | 4.5 % Show Supplier Material materials with Elongación of 4.5 % | ISO 527 | yield | ||
Hardness, Rockwell L | 23.0 °C | 92 [-] Show Supplier Material materials with Hardness, Rockwell L of 92 [-] | ASTM D 785 | ||
Impact strength, Izod notched, ASTM | 23.0 °C | 753 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 753 J/m | ASTM D 256 | notched, 23°C | ||
Instrumented Impact, Total Energy | 23.0 °C | 62 J Show Supplier Material materials with Instrumented Impact, Total Energy of 62 J | ASTM D 3763 | -30°C | ||
Módulo de flexión | 23.0 °C | 2.3 GPa Show Supplier Material materials with Módulo de flexión of 2.3 GPa | ISO 178 | 2 mm/min | ||
Módulo elástico | 23.0 °C | 2.4 GPa Show Supplier Material materials with Módulo elástico of 2.4 GPa | ISO 527 | 1 mm/min | ||
Resistencia a la flexión | 23.0 °C | 93 MPa Show Supplier Material materials with Resistencia a la flexión of 93 MPa | ISO 178 | break, 2 mm/min | ||
Resistencia a la tracción | 23.0 °C | 47 MPa Show Supplier Material materials with Resistencia a la tracción of 47 MPa | ISO 527 | break | ||
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 55 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 55 kJ/m² | ISO 179/2C | 23°C | ||
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 51 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 51 kJ/m² | ISO 180/1A | 80*10*4, 23°C | ||
Impact strength, Izod unnotched, ASTM | ASTM D 4812 | 23°C | ||||
Resistencia al choque, ensayo Charpy no entallado | ISO 179/2C | 23°C | ||||
Resistencia al choque, ensayo Izod no entallado | ISO 180/1U | 80*10*4, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 6.5E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 6.5E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 6.6E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 6.6E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Heat deflection temperature, 0.45 MPa | 110 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 110 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 103 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 103 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |||
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |||
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |||
Temperatura de flexión bajo carga | 103 - 110 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 103 - 110 °C | ||||
Temperatura de reblandecimiento Vicat | 119 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 119 °C | ISO 306 | Rate B/120 | |||
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=104263180- - <br> UL Recognized, 94HB Flame Class Rating: ≥0.4mm UL 94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 1GHz | 23.0 °C | 2.8 [-] Show Supplier Material materials with Dielectric constant, 1GHz of 2.8 [-] | SABIC method | 1.1 GHz |
Dissipation factor, 1GHz | 23.0 °C | 6E-3 [-] Show Supplier Material materials with Dissipation factor, 1GHz of 6E-3 [-] | SABIC method | |
Sheet resistivity, ROA | 23.0 °C | 1.00E+16 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+16 Ω | >, ASTM D 257 |
Volume resistivity | 23.0 °C | 1.00E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+16 Ω·cm | >, ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.6 % Show Supplier Material materials with Contracción of 0.6 % | ASTM D 955 | 24 hrs |
Contracción transversal | 23.0 °C | 0.6 % Show Supplier Material materials with Contracción transversal of 0.6 % | ASTM D 955 | 24 hrs |
Velocidad de flujo de la masa derretida | 20 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 20 g/10min | ASTM D 1238 | 300°C/1.2 kgf |
Technological properties
Property | ||
---|---|---|
Application areas | Monitoring and Imaging, Power Manangement, Wireless Communications, Wiring Devices, Industrial Material Handling, Electronic Components, Electronics, Enclosures | |
Availability | Asia | |
Processing methods | Drying Temperature: 100°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |