General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad relativa | 23.0 °C | 1.02 [-] Show Supplier Material materials with Densidad relativa of 1.02 [-] | ASTM D 792 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Temperatura de transición del vidrio | 160 °C Show Supplier Material materials with Temperatura de transición del vidrio of 160 °C | SABIC method | (half width) |
Eléctrico
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Viscosidad | 23.0 °C | 0.16 Pa·s Show Supplier Material materials with Viscosidad of 0.16 Pa·s | SABIC method | 50 wt% in methyl ethyl ketone, 25°C |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Material, Electronic Material Handling, Additive Plastic, Composite, Circuit Board, Data Transfer | |
Availability | Europe,Asia,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |