Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.33 % Show Supplier Material materials with Absorción de agua of 0.33 % | ISO 62-1 | (23°C/saturated) |
Densidad | 23.0 °C | 1.19 g/cm³ Show Supplier Material materials with Densidad of 1.19 g/cm³ | ISO 1183 |
Densidad relativa | 23.0 °C | 1.18 [-] Show Supplier Material materials with Densidad relativa of 1.18 [-] | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.15 % Show Supplier Material materials with Moisture absorption of 0.15 % | ISO 62 | (23°C / 50% RH) |
Índice límite de óxigeno | 23.0 °C | 31 % Show Supplier Material materials with Índice límite de óxigeno of 31 % |
Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Elongación | 23.0 °C | 5.2 % Show Supplier Material materials with Elongación of 5.2 % | ISO 527 | yield, 50 mm/min | ||
Hardness, Ball Indentation | 23.0 °C | 95 MPa Show Supplier Material materials with Hardness, Ball Indentation of 95 MPa | ISO 2039-1 | H358/30 | ||
Impact strength, Izod notched, ASTM | 23.0 °C | 750 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 750 J/m | ASTM D 256 | ||
Instrumented Impact, Total Energy | 23.0 °C | 69 J Show Supplier Material materials with Instrumented Impact, Total Energy of 69 J | ASTM D 3763 | 23°C | ||
Módulo de flexión | 23.0 °C | 2.3 GPa Show Supplier Material materials with Módulo de flexión of 2.3 GPa | ISO 178 | 2 mm/min | ||
Módulo elástico | 23.0 °C | 2.2 GPa Show Supplier Material materials with Módulo elástico of 2.2 GPa | ISO 527 | 1 mm/min | ||
Resistencia a la flexión | 23.0 °C | 86 MPa Show Supplier Material materials with Resistencia a la flexión of 86 MPa | ISO 178 | yield, 2 mm/min | ||
Resistencia a la tracción | 23.0 °C | 57 MPa Show Supplier Material materials with Resistencia a la tracción of 57 MPa | ISO 527 | yield, 50 mm/min | ||
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 24 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 24 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*3 sp=62mm, -30°C | ||
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 21 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 21 kJ/m² | ISO 180/1A | notched 80*10*3, -30°C | ||
Resistencia al choque, ensayo Charpy no entallado | ISO 179/1eU | Unnotch Edgew 80*10*3 sp=62mm, -30°C | ||||
Resistencia al choque, ensayo Izod no entallado | ISO 180/1U | 80*10*3, -30°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball Pressure Test | nan | IEC 60695-10-2 | 125°C +/- 2°C | |||
Coeficiente de dilatación térmica | 23.0 °C | 7.5E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7.5E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 7.5E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 7.5E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Glow Wire Ignition Temperature | 875 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 875 °C | IEC 60695-2-13 | 3.0 mm | |||
Heat deflection temperature, 0.45 MPa | 135 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 135 °C | ISO 75/Be | edgew. Annealed 80°C, 4 hrs | |||
Heat deflection temperature, 1.80 MPa | 125 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 125 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |||
Temperatura de flexión bajo carga | 125 - 135 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 125 - 135 °C | ||||
Temperatura de reblandecimiento Vicat | 143 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 143 °C | ISO 306 | Rate B/50 | |||
Inflamabilidad | Glow Wire Flammability Index 850°C, passes at: 1mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 3mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 3mm IEC 60695-2-12 <br> Glow Wire Ignitability Temperature, 1.0 mm: 875°C IEC 60695-2-13 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.4 % Show Supplier Material materials with Contracción of 0.4 % | SABIC method | 3.2 mm |
Contracción transversal | 23.0 °C | 0.4 % Show Supplier Material materials with Contracción transversal of 0.4 % | SABIC method | 3.2 mm |
Velocidad de flujo de la masa derretida | 17 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 17 g/10min | ASTM D 1238 | 300°C/1.2 kgf | |
Velocidad de flujo del volumen derretido | 16 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 16 cm³/10min | ISO 1133 | MVR at 300°C/1.2 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Wearables, Wireless Communications, Small Appliance, Photo/Video Camera, Medical Facility Infrastructure, Personal Computing, Circuit Protection, Data Transfer, Data Management, Enclosures, Enclosure/Housing/Cover, Electronic Components | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |