General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 4.5 % Show Supplier Material materials with Absorción de agua of 4.5 % | ISO 62-1 | (23°C/saturated) |
Densidad | 23.0 °C | 1.56 g/cm³ Show Supplier Material materials with Densidad of 1.56 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2.5 % Show Supplier Material materials with Elongación of 2.5 % | ISO 527 | break, 5 mm/min |
Módulo de flexión | 23.0 °C | 6 GPa Show Supplier Material materials with Módulo de flexión of 6 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 6.2 GPa Show Supplier Material materials with Módulo elástico of 6.2 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 140 MPa Show Supplier Material materials with Resistencia a la flexión of 140 MPa | ISO 178 | break, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 85 MPa Show Supplier Material materials with Resistencia a la tracción of 85 MPa | ISO 527 | break, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 5 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 3E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 3E-5 1/K | ISO 11359-2 | 23°C to 60°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 3E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 3E-5 1/K | ISO 11359-2 | 23°C to 60°C | ||
Heat deflection temperature, 0.45 MPa | 245 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 245 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |||
Heat deflection temperature, 1.80 MPa | 175 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 175 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |||
Temperatura de flexión bajo carga | 175 - 245 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 175 - 245 °C | ||||
Temperatura de reblandecimiento Vicat | 255 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 255 °C | ISO 306 | Rate A/50 | |||
Inflamabilidad | UL Compliant, 94HB Flame Class Rating: 1.6mm UL 94 by SABIC-IP |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Índice de seguimiento comparativo | 23.0 °C | 400 V Show Supplier Material materials with Índice de seguimiento comparativo of 400 V | IEC 60112 | M |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 % Show Supplier Material materials with Contracción of 0.5 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 75 to 85.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |