General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad relativa | 23.0 °C | 1.18 [-] Show Supplier Material materials with Densidad relativa of 1.18 [-] | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 50 % Show Supplier Material materials with Elongación of 50 % | ASTM D 638 | break |
Módulo de flexión | 23.0 °C | 2.7 GPa Show Supplier Material materials with Módulo de flexión of 2.7 GPa | ASTM D 790 |
Resistencia a la flexión | 23.0 °C | 103 MPa Show Supplier Material materials with Resistencia a la flexión of 103 MPa | ASTM D 790 |
Resistencia a la tracción | 23.0 °C | 66 MPa Show Supplier Material materials with Resistencia a la tracción of 66 MPa | ASTM D 638 | yield |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Relative temperature index, electrical | 85 °C Show Supplier Material materials with Relative temperature index, electrical of 85 °C | UL 746B | |
Relative temperature index, mechanical impact | 85 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 85 °C | UL 746B | |
Relative temperature index, mechanical strength | 85 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 85 °C | UL 746B | |
Inflamabilidad | UL Recognized, 94HB Flame Class Rating: ≥0.7mm UL 94 <br> UL Recognized, 94V-1 Flame Class Rating: ≥1.2mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥1.5mm UL 94 <br> UL Recognized, 94-5VA Flame Class Rating: ≥3.4mm UL 94 <br> UL Recognized, 94-5VB Flame Class Rating: ≥2.0mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=104340779- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica, 1 MHz | 23.0 °C | 2.7 [-] Show Supplier Material materials with Constante dieléctrica, 1 MHz of 2.7 [-] | IEC 60250 |
Dielectric constant, 60Hz | 23.0 °C | 2.8 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 2.8 [-] | IEC 60250 |
Dissipation factor, 1MHz | 23.0 °C | 8E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 8E-3 [-] | IEC 60250 |
Dissipation factor, 50Hz | 23.0 °C | 4E-3 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 4E-3 [-] | IEC 60250 | 50/60 Hz |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
High Volt Arc Track Rate | 23.0 °C | 2 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 2 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 3 mm Show Supplier Material materials with Hot-Wire Ignition of 3 mm | ≥, UL 746A | PLC 2 |
Rigidez dieléctrica | 23.0 °C | 430 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 430 kV/mm | IEC 60243-1 | in oil, 3.2 mm, |
Sheet resistivity, ROA | 23.0 °C | 1.00E+15 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+15 Ω | ASTM D 257 |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm | ASTM D 257 |
Índice de seguimiento comparativo | 23.0 °C | 2 V Show Supplier Material materials with Índice de seguimiento comparativo of 2 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.4 % Show Supplier Material materials with Contracción of 0.4 % | SABIC method |
Contracción transversal | 23.0 °C | 0.4 % Show Supplier Material materials with Contracción transversal of 0.4 % | SABIC method |
Velocidad de flujo de la masa derretida | 17 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 17 g/10min | ASTM D 1238 | 260°C/2.16 kgf |
Technological properties
Property | ||
---|---|---|
Application areas | Medical Facility Infrastructure | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80 to 90.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |