Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.328 g/cm³ Show Supplier Material materials with Densidad of 1.328 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 1 % Show Supplier Material materials with Moisture absorption of 1 % | ASTM D 570 | (50% RH, Equilibrium) |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Módulo de flexión | 23.0 °C | 8.6 GPa Show Supplier Material materials with Módulo de flexión of 8.6 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Resistencia a la flexión | 23.0 °C | 248 MPa Show Supplier Material materials with Resistencia a la flexión of 248 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.98E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.98E-5 1/K | ASTM E 831 | -20°C to 150°C | ||
Temperatura de reblandecimiento Vicat | 248 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 248 °C | ASTM D 1525 | Rate B/50 | |||
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=104248654- - <br> UL Recognized, 94HB Flame Class Rating: ≥1.5mm UL 94 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Non-LED Lighting, Personal Care, Medical Device, Meter Water, Interior Rail Components, Pump, Power Boat, Pallet, Recreational Vehicle, Plumbing, Photovoltaic Components, Power Manangement, Sensor, Small Appliance, Respiratory, Washing Machine, Underhood, Tray, Swimming Pool/Spa, Wireless Communications, Weaving Machine, Water Treatment/Filtration, Weapon, Wiring Devices, Electronic Components, Energy Management, Electronics, Enclosures, Heavy Vehicles, Gas/Electric Oven, Food Processor, Fixture Bath/Shower, Engine Cooling System, Electrical, Engine Component, Auto Aftermarket, Auto Electrical, Building Accessory, Circuit Protection, Air Cabin Interiors, Defense Vehicles, Displays, Cooking Range, Data Management | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 95 to 105.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |