General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.98 % Show Supplier Material materials with Absorción de agua of 0.98 % | ASTM D 570 | (23°C/Saturated) |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 3.5 % Show Supplier Material materials with Elongación of 3.5 % | ASTM D 638 | brk, Type I, 5 mm/min |
Módulo de flexión | 23.0 °C | 6.6 GPa Show Supplier Material materials with Módulo de flexión of 6.6 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Módulo elástico | 23.0 °C | 6 GPa Show Supplier Material materials with Módulo elástico of 6 GPa | ASTM D 638 | 5 mm/min |
Resistencia a la flexión | 23.0 °C | 179 MPa Show Supplier Material materials with Resistencia a la flexión of 179 MPa | ASTM D 790 | brk, 2.6 mm/min, 100 mm span |
Resistencia a la tracción | 23.0 °C | 103 MPa Show Supplier Material materials with Resistencia a la tracción of 103 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 32 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 32 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 2.34E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.34E-5 1/K | ASTM E 831 | -20°C to 150°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 2.7E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 2.7E-5 1/K | ASTM E 831 | -20°C to 150°C | ||
Heat deflection temperature, 1.80 MPa | 207 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 207 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Relative temperature index, electrical | 170 °C Show Supplier Material materials with Relative temperature index, electrical of 170 °C | UL 746B | |||
Relative temperature index, mechanical impact | 170 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 170 °C | UL 746B | |||
Relative temperature index, mechanical strength | 170 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 170 °C | UL 746B | |||
Temperatura de flexión bajo carga | 207 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 207 °C | ||||
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221100- - <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.81mm UL 94 <br> Glow Wire Flammability Index, 1.5 mm: 960°C IEC 60695-2-12 <br> Glow Wire Ignitability Temperature, 1.5 mm: 875°C IEC 60695-2-13 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica, 1 MHz | 23.0 °C | 3.49 [-] Show Supplier Material materials with Constante dieléctrica, 1 MHz of 3.49 [-] | ASTM D 150 |
High Amp Arc Ignition | 23.0 °C | 3 mm Show Supplier Material materials with High Amp Arc Ignition of 3 mm | ≥, UL 746A | PLC 3 |
High Volt Arc Track Rate | 23.0 °C | 0 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 0 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 0.81 mm Show Supplier Material materials with Hot-Wire Ignition of 0.81 mm | ≥, UL 746A | PLC 2 |
Índice de seguimiento comparativo | 23.0 °C | 4 V Show Supplier Material materials with Índice de seguimiento comparativo of 4 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.2 % Show Supplier Material materials with Contracción of 0.2 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Application areas | Pump, Non-LED Lighting, Enclosures, Forward Lighting, Lab Ware and Clinical Diagnostics, Heavy Vehicles | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 150°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |