General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad relativa | 23.0 °C | 1.01 [-] Show Supplier Material materials with Densidad relativa of 1.01 [-] | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore A | 23.0 °C | 84 [-] Show Supplier Material materials with Dureza Shore A of 84 [-] | ASTM D 2240 | 30S reading |
Elongación | 23.0 °C | 175 % Show Supplier Material materials with Elongación of 175 % | ISO 527 | break, 50 mm/min |
Módulo de flexión | 23.0 °C | 0.1 GPa Show Supplier Material materials with Módulo de flexión of 0.1 GPa | ISO 178 | 12.5 mm/min |
Resistencia a la tracción | 23.0 °C | 7 MPa Show Supplier Material materials with Resistencia a la tracción of 7 MPa | ISO 527 | break, 50 mm/min |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Brittleness temperature | -40 °C Show Supplier Material materials with Brittleness temperature of -40 °C | <, ASTM D 746 | |
Glow Wire Ignition Temperature | 750 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 750 °C | IEC 60695-2-13 | 3.0 mm | |
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101939210- - <br> UL Recognized, 94HB Flame Class Rating: ≥0.6mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥6mm UL 94 <br> Glow Wire Flammability Index 750°C, passes at: 3mm IEC 60695-2-12 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Volume resistivity | 23.0 °C | 7.10E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 7.10E+15 Ω·cm | ASTM D 257 |
Índice de seguimiento comparativo | 23.0 °C | 0 V Show Supplier Material materials with Índice de seguimiento comparativo of 0 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.95 % Show Supplier Material materials with Contracción of 0.95 % | ASTM D 955 | 24 hrs |
Contracción transversal | 23.0 °C | 0.75 % Show Supplier Material materials with Contracción transversal of 0.75 % | ASTM D 955 | 24 hrs |
Velocidad de flujo de la masa derretida | 24 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 24 g/10min | ASTM D 1238 | 210°C/5 kgf |
Technological properties
Property | ||
---|---|---|
Application areas | Wire & cable | |
Availability | Asia,Americas | |
Processing methods | Drying Temperature: 60 to 80.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |