General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.22 % Show Supplier Material materials with Absorción de agua of 0.22 % | ISO 62-1 | (23°C/saturated) |
Densidad relativa | 23.0 °C | 1.16 [-] Show Supplier Material materials with Densidad relativa of 1.16 [-] | ASTM D 792 |
Índice límite de óxigeno | 23.0 °C | 30 % Show Supplier Material materials with Índice límite de óxigeno of 30 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2.5 % Show Supplier Material materials with Elongación of 2.5 % | ISO 527 | yield, 5 mm/min |
Módulo de flexión | 23.0 °C | 3 GPa Show Supplier Material materials with Módulo de flexión of 3 GPa | ISO 178 | 2 mm/min |
Resistencia a la flexión | 23.0 °C | 110 MPa Show Supplier Material materials with Resistencia a la flexión of 110 MPa | ISO 178 | yield, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 75 MPa Show Supplier Material materials with Resistencia a la tracción of 75 MPa | ISO 527 | yield, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 6 kJ/m² | ISO 180/1A | notched 80*10*4, -30°C |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 135 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 135 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |
Relative temperature index, electrical | 110 °C Show Supplier Material materials with Relative temperature index, electrical of 110 °C | UL 746B | |
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |
Relative temperature index, mechanical strength | 110 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 110 °C | UL 746B | |
Temperatura de flexión bajo carga | 135 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 135 °C | ||
Temperatura de reblandecimiento Vicat | 145 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 145 °C | ISO 306 | Rate B/120 | |
Inflamabilidad | Glow Wire Ignitability Temperature, 1.0 mm: 775°C IEC 60695-2-13 <br> Needle Flame Test, 10 s , passes at: 1.5mm IEC 60695-2-2 <br> UL Recognized, 94V-1 Flame Class Rating: ≥0.8mm UL 94 <br> Glow Wire Flammability Index, 1.0 mm: 960°C IEC 60695-2-12 <br> Glow Wire Flammability Index, 1.5 mm: 960°C IEC 60695-2-12 <br> Glow Wire Ignitability Temperature, 1.5 mm: 775°C IEC 60695-2-13 <br> UL Recognized, 94-5VA Flame Class Rating: ≥2.5mm UL 94 <br> UV-light, water exposure/immersion: F2- UL 746C <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=306538- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica, 1 MHz | 23.0 °C | 2.7 [-] Show Supplier Material materials with Constante dieléctrica, 1 MHz of 2.7 [-] | IEC 60250 |
Dielectric constant, 60Hz | 23.0 °C | 2.8 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 2.8 [-] | IEC 60250 | 50/60 Hz |
Dissipation factor, 1MHz | 23.0 °C | 3E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 3E-3 [-] | IEC 60250 |
Dissipation factor, 50Hz | 23.0 °C | 5E-3 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 5E-3 [-] | IEC 60250 | 50/60 Hz |
High Amp Arc Ignition | 23.0 °C | 0.8 mm Show Supplier Material materials with High Amp Arc Ignition of 0.8 mm | ≥, UL 746A | PLC 1 |
High Volt Arc Track Rate | 23.0 °C | 4 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 0.8 mm Show Supplier Material materials with Hot-Wire Ignition of 0.8 mm | ≥, UL 746A | PLC 1 |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm | IEC 60093 | |
Índice de seguimiento comparativo | 23.0 °C | 2 V Show Supplier Material materials with Índice de seguimiento comparativo of 2 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.3 % Show Supplier Material materials with Contracción of 0.3 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Circuit Protection, Building Accessory, Auto Electrical, Battery Pack, Audio, Auto Aftermarket, Aerospace, Coffee Maker/Espresso Machine, Cladding/Roof, Document Handling, Displays, Dishwasher, Enclosures, Enclosure/Housing/Cover, Energy Management, Electronic Components, Humidity Control, Individual Equiptment, Eyeglasses, Freezer, Fixture Bath/Shower, Engine Component, EV/HEV Battery, Wiring Devices, Wireless Communications, Personal Computing, Monitoring and Imaging, Meter Gas, Medical Device, Respiratory, Plumbing, Photovoltaic Components, Power Manangement, Pump | |
Availability | Europe,Asia,Americas | |
Processing methods | Nozzle Temperature: 260 to 280.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |