General
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 15 % Show Supplier Material materials with Elongación of 15 % | ASTM D 638 | brk, Type I, 50 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 106 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 106 J/m | ASTM D 256 | notched, -30°C |
Módulo de flexión | 23.0 °C | 2.4 GPa Show Supplier Material materials with Módulo de flexión of 2.4 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Resistencia a la flexión | 23.0 °C | 100 MPa Show Supplier Material materials with Resistencia a la flexión of 100 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Resistencia a la tracción | 23.0 °C | 53 MPa Show Supplier Material materials with Resistencia a la tracción of 53 MPa | ASTM D 638 | brk, Type I, 50 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 180 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 180 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||
Glow Wire Ignition Temperature | 725 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 725 °C | IEC 60695-2-13 | 2.0 mm | |
Heat deflection temperature, 0.45 MPa | 126 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 126 °C | ASTM D 648 | 6.4 mm, unannealed | |
Heat deflection temperature, 1.80 MPa | 118 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 118 °C | ASTM D 648 | 6.4 mm, unannealed | |
Relative temperature index, electrical | 110 °C Show Supplier Material materials with Relative temperature index, electrical of 110 °C | UL 746B | |
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |
Relative temperature index, mechanical strength | 110 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 110 °C | UL 746B | |
Temperatura de flexión bajo carga | 118 - 126 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 118 - 126 °C | ||
Inflamabilidad | UL Recognized, 94V-0 Flame Class Rating: ≥6mm UL 94 <br> UL Recognized, 94V-1 Flame Class Rating: ≥1.5mm UL 94 <br> UV-light, water exposure/immersion: F1- UL 746C <br> Radiant Panel Listing: RP100- UL Tested <br> Glow Wire Flammability Index, 1.0 mm: 900°C IEC 60695-2-12 <br> Glow Wire Flammability Index, 1.5 mm: 900°C IEC 60695-2-12 <br> Glow Wire Ignitability Temperature, 1.0 mm: 700°C IEC 60695-2-13 <br> Glow Wire Ignitability Temperature, 1.5 mm: 700°C IEC 60695-2-13 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100107130- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica, 1 MHz | 23.0 °C | 2.46 [-] Show Supplier Material materials with Constante dieléctrica, 1 MHz of 2.46 [-] | ASTM D 150 |
Dielectric constant, 60Hz | 23.0 °C | 2.52 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 2.52 [-] | ASTM D 150 | 50/60 Hz |
Dissipation factor, 1MHz | 23.0 °C | 2.1E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 2.1E-3 [-] | ASTM D 150 |
Dissipation factor, 50Hz | 23.0 °C | 3.4E-3 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 3.4E-3 [-] | ASTM D 150 | 50/60 Hz |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
High Volt Arc Track Rate | 23.0 °C | 4 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
Rigidez dieléctrica | 23.0 °C | 18.1 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 18.1 kV/mm | ASTM D 149 | in oil, 3.2 mm |
Sheet resistivity, ROA | 23.0 °C | 1.00E+15 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+15 Ω | >, ASTM D 257 |
Volume resistivity | 23.0 °C | 2.30E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 2.30E+16 Ω·cm | ASTM D 257 |
Índice de seguimiento comparativo | 23.0 °C | 1 V Show Supplier Material materials with Índice de seguimiento comparativo of 1 V | UL 746A | (UL) {PLC} |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Air Conditioning, Aerospace, Circuit Protection, Auto Electrical, ATM/Ticket Machine, Auto Aftermarket, Displays, Document Handling, Building Element, Data Transfer, Data Management, Electronic Components, Enclosure/Housing/Cover, Electronics, Energy Management, Enclosures, Lab Ware and Clinical Diagnostics, Lawn/Garden, Hot Water System, Head Protection, Gear/Bearing/Slider, Fixture Bath/Shower, Food Processor, Electronic Material Handling, Wiring Devices, Wireless Communications, Washing Machine, Vending Machine, Personal Computing, Non-LED Lighting, Medical Device, LED Lighting, Microwave Oven, Laundry Dryer, Monitoring and Imaging, Small Appliance, Surgical Devices, Safety Glasses, Security/Detection, Refrigerator, Pump, Photovoltaic Components, Power Manangement | |
Availability | Asia,Americas | |
Processing methods | Nozzle Temperature: 280 to 310.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |