General
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 5 % Show Supplier Material materials with Elongación of 5 % | ASTM D 638 | brk, Type I, 5 mm/min |
Módulo de flexión | 23.0 °C | 7.8 GPa Show Supplier Material materials with Módulo de flexión of 7.8 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Resistencia a la flexión | 23.0 °C | 172 MPa Show Supplier Material materials with Resistencia a la flexión of 172 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Resistencia a la tracción | 23.0 °C | 120 MPa Show Supplier Material materials with Resistencia a la tracción of 120 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 2.52E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.52E-5 1/K | ASTM E 831 | -40°C to 95°C | ||
Heat deflection temperature, 0.45 MPa | 140 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 140 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Heat deflection temperature, 1.80 MPa | 135 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 135 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Relative temperature index, electrical | 110 °C Show Supplier Material materials with Relative temperature index, electrical of 110 °C | UL 746B | |||
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |||
Relative temperature index, mechanical strength | 110 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 110 °C | UL 746B | |||
Temperatura de flexión bajo carga | 135 - 140 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 135 - 140 °C | ||||
Inflamabilidad | UL Recognized, 94V-1 Flame Class Rating: ≥0.71mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=228591- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=237105- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 60Hz | 23.0 °C | 3.15 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 3.15 [-] | ASTM D 150 | 50/60 Hz |
Dissipation factor, 50Hz | 23.0 °C | 2E-3 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 2E-3 [-] | ASTM D 150 | 50/60 Hz |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 2 |
High Volt Arc Track Rate | 23.0 °C | 4 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
Rigidez dieléctrica | 23.0 °C | 20.8 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 20.8 kV/mm | ASTM D 149 | in oil, 3.2 mm |
Índice de seguimiento comparativo | 23.0 °C | 3 V Show Supplier Material materials with Índice de seguimiento comparativo of 3 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.1 % Show Supplier Material materials with Contracción of 0.1 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Circuit Protection, Building Accessory, Cladding/Roof, Document Handling, Enclosures, Enclosure/Housing/Cover, Electronic Components, Hot Water System, Lawn/Garden, Fixture Bath/Shower, Furnace/Heater, Electronic Material Handling, Washing Machine, Wiring Devices, Wireless Communications, Motorcycle, Personal Care, Medical Device, LED Lighting, Surgical Devices, Small Appliance, Security/Detection, Renal and Blood Handling, Pump, Refrigerator | |
Availability | Europe,Asia,Americas | |
Processing methods | Mold Temperature: 80 to 110.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |