General
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 5 % Show Supplier Material materials with Elongación of 5 % | ASTM D 638 | brk, Type I, 5 mm/min |
Módulo de flexión | 23.0 °C | 5.7 GPa Show Supplier Material materials with Módulo de flexión of 5.7 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Resistencia a la flexión | 23.0 °C | 151 MPa Show Supplier Material materials with Resistencia a la flexión of 151 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Resistencia a la tracción | 23.0 °C | 106 MPa Show Supplier Material materials with Resistencia a la tracción of 106 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 3.6E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 3.6E-5 1/K | ASTM E 831 | -40°C to 95°C | ||
Heat deflection temperature, 0.45 MPa | 137 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 137 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Heat deflection temperature, 1.80 MPa | 132 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 132 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Relative temperature index, electrical | 110 °C Show Supplier Material materials with Relative temperature index, electrical of 110 °C | UL 746B | |||
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |||
Relative temperature index, mechanical strength | 110 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 110 °C | UL 746B | |||
Temperatura de flexión bajo carga | 132 - 137 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 132 - 137 °C | ||||
Inflamabilidad | UL Recognized, 94V-0 Flame Class Rating: ≥6mm UL 94 <br> UL Recognized, 94-5VA Flame Class Rating: ≥2mm UL 94 <br> UL Recognized, 94V-1 Flame Class Rating: ≥1.5mm UL 94 <br> Glow Wire Flammability Index, 1.0 mm: 960°C IEC 60695-2-12 <br> Glow Wire Flammability Index, 1.5 mm: 960°C IEC 60695-2-12 <br> Glow Wire Ignitability Temperature, 1.0 mm: 775°C IEC 60695-2-13 <br> Glow Wire Ignitability Temperature, 1.5 mm: 750°C IEC 60695-2-13 <br> UV-light, water exposure/immersion: F1- UL 746C <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=600331- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=624509- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 2 |
High Volt Arc Track Rate | 23.0 °C | 3 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 3 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
Rigidez dieléctrica | 23.0 °C | 23.6 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 23.6 kV/mm | ASTM D 149 | in oil, 3.2 mm |
Índice de seguimiento comparativo | 23.0 °C | 3 V Show Supplier Material materials with Índice de seguimiento comparativo of 3 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.2 % Show Supplier Material materials with Contracción of 0.2 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Pump, Pipe/Fitting, Power Manangement, Photovoltaic Components, Plumbing, Respiratory, Security/Detection, Sensor, Surgical Devices, Meter Gas, Ignition System, Meter Water, Microwave Oven, Personal Computing, Motorcycle, Non-LED Lighting, Wireless Communications, Wiring Devices, Water Treatment/Filtration, Wearables, Washing Machine, Travel Suitcase, Traffic Management, Swimming Pool/Spa, EV/HEV Battery, Electronic Material Handling, EV Infrastructure, Fixture Bath/Shower, Individual Equiptment, Industrial Material Handling, HVAC Underhood, Hygiene/Personal Care, Lab Ware and Clinical Diagnostics, Humidity Control, Hot Water System, Heavy Vehicles, Electronic Components, Energy Management, Electronics, Enclosure/Housing/Cover, Enclosures, Dishwasher, Defense Vehicles, Drain Pan, Displays, Document Handling, Cluster, Coffee Maker/Espresso Machine, Building Element, Battery System, Data Transfer, Air Conditioning, Auto Aftermarket, Audio, ATM/Ticket Machine, Battery Pack, Building Accessory, Circuit Protection | |
Availability | Europe,Asia,Americas | |
Processing methods | Rear - Zone 1 Temperature: 265 to 315.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |