General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.46 g/cm³ Show Supplier Material materials with Densidad of 1.46 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.04 % Show Supplier Material materials with Moisture absorption of 0.04 % | ISO 62 | (23°C / 50% RH) |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 1.8 % Show Supplier Material materials with Elongación of 1.8 % | ISO 527 | break, 5 mm/min |
Flexural strain | 23.0 °C | 2.8 % Show Supplier Material materials with Flexural strain of 2.8 % | ISO 178 | break, 2 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 44 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 44 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 330 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 330 J/m | ASTM D 4812 | unnotched, -30°C |
Instrumented Impact, Total Energy | 23.0 °C | 11 J Show Supplier Material materials with Instrumented Impact, Total Energy of 11 J | ASTM D 3763 | 23°C |
Módulo de flexión | 23.0 °C | 5.3 GPa Show Supplier Material materials with Módulo de flexión of 5.3 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Módulo elástico | 23.0 °C | 5.8 GPa Show Supplier Material materials with Módulo elástico of 5.8 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 105 MPa Show Supplier Material materials with Resistencia a la flexión of 105 MPa | ISO 178 | yield, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 62 MPa Show Supplier Material materials with Resistencia a la tracción of 62 MPa | ISO 527 | break, 5 mm/min |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 7 kJ/m² | ISO 179/1eA | V-notch Edgew, 23°C, 80*10*4 sp=62mm |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 5 kJ/m² | ISO 180/1A | notched 80*10*4, -30°C |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 21 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod no entallado of 21 kJ/m² | ISO 180/1U | unnotched 80*10*4 |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 2.9E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.9E-5 1/K | ISO 11359-2 | 23°C to 60°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 7.4E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 7.4E-5 1/K | ISO 11359-2 | 23°C to 60°C | ||
Heat deflection temperature, 1.80 MPa | 96 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 96 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 60 °C Show Supplier Material materials with Relative temperature index, electrical of 60 °C | UL 746B | |||
Relative temperature index, mechanical impact | 60 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 60 °C | UL 746B | |||
Relative temperature index, mechanical strength | 60 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 60 °C | UL 746B | |||
Temperatura de flexión bajo carga | 96 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 96 °C | ||||
Temperatura de reblandecimiento Vicat | 105 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 105 °C | ISO 306 | Rate B/120 | |||
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101282735- - <br> UL Recognized, 94V-0 Flame Class Rating: 1.5mm UL 94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 1000 - 1000000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1000 - 1000000 Ω | ASTM D 257 |
Shielding effectiveness | 23.0 °C | 47 dB Show Supplier Material materials with Shielding effectiveness of 47 dB | SABIC method | @ 1.5mm |
Volume resistivity | 23.0 °C | 10000 - 1000000 Ω·cm Show Supplier Material materials with Volume resistivity of 10000 - 1000000 Ω·cm | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Personal Computing, Personal Care, Wireless Communications, Data Management, Document Handling, Displays, Enclosures | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 85 to 90.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |