General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.25 g/cm³ Show Supplier Material materials with Densidad of 1.25 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Elongación | 23.0 °C | 20 % Show Supplier Material materials with Elongación of 20 % | ASTM D 638 | break | ||
Impact strength, Izod notched, ASTM | 23.0 °C | 106 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 106 J/m | ASTM D 256 | ||
Módulo de flexión | 23.0 °C | 2.8 GPa Show Supplier Material materials with Módulo de flexión of 2.8 GPa | ASTM D 790 | ||
Módulo elástico | 23.0 °C | 2.8 GPa Show Supplier Material materials with Módulo elástico of 2.8 GPa | ASTM D 638 | 50 mm/min | ||
Resistencia a la flexión | 23.0 °C | 96 MPa Show Supplier Material materials with Resistencia a la flexión of 96 MPa | ASTM D 790 | ||
Resistencia a la tracción | 23.0 °C | 58 MPa Show Supplier Material materials with Resistencia a la tracción of 58 MPa | ASTM D 638 | yield | ||
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 106 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 106 kJ/m² | ASTM D 256 | notched, 23°C | ||
Impact strength, Izod unnotched, ASTM | ASTM D 4812 | 23°C |
Aplicaciones térmicas
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 1.00E+4 - 1.00E+7 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+4 - 1.00E+7 Ω | ASTM D 257 |
Volume resistivity | 23.0 °C | 1.00E+4 - 1.00E+7 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+4 - 1.00E+7 Ω·cm | ASTM D 257 |
Technological properties
Property | ||
---|---|---|
Application areas | Semiconductor | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |