Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.26 g/cm³ Show Supplier Material materials with Densidad of 1.26 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 9 % Show Supplier Material materials with Elongación of 9 % | ISO 527 | break, 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 180 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 180 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 1600 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1600 J/m | ASTM D 4812 | 23°C |
Módulo de flexión | 23.0 °C | 2.4 GPa Show Supplier Material materials with Módulo de flexión of 2.4 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 2.4 GPa Show Supplier Material materials with Módulo elástico of 2.4 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 88 MPa Show Supplier Material materials with Resistencia a la flexión of 88 MPa | ISO 178 | break, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 44 MPa Show Supplier Material materials with Resistencia a la tracción of 44 MPa | ISO 527 | break, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 10 kJ/m² | ISO 180/1A | notched 80*10*4, -40°C |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 130 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod no entallado of 130 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 5E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 5E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 5E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 5E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Heat deflection temperature, 1.80 MPa | 124 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 124 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |||
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |||
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |||
Temperatura de flexión bajo carga | 124 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 124 °C | ||||
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101283809- - <br> UL Recognized, 94V-1 Flame Class Rating: 2.5mm UL 94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 1.00E+6 - 1.00E+10 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+6 - 1.00E+10 Ω | ASTM D 257 |
Volume resistivity | 23.0 °C | 1.00E+6 - 1.00E+10 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+6 - 1.00E+10 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 % Show Supplier Material materials with Contracción of 0.5 % | SABIC method |
Contracción transversal | 23.0 °C | 0.5 % Show Supplier Material materials with Contracción transversal of 0.5 % | SABIC method |
Velocidad de flujo de la masa derretida | 55 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 55 g/10min | ASTM D 1238 | 300°C/10 kgf | |
Velocidad de flujo del volumen derretido | 50 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 50 cm³/10min | ISO 1133 | MVR at 300°C/10.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Data Transfer, Data Management, Enclosure/Housing/Cover | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |