General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.15 g/cm³ Show Supplier Material materials with Densidad of 1.15 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 13.5 % Show Supplier Material materials with Elongación of 13.5 % | ASTM D 638 | break |
Impact strength, Izod notched, ASTM | 23.0 °C | 150 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 150 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 1810 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1810 J/m | ASTM D 4812 | 23°C |
Módulo de flexión | 23.0 °C | 2.6 GPa Show Supplier Material materials with Módulo de flexión of 2.6 GPa | ASTM D 790 |
Módulo elástico | 23.0 °C | 2.1 GPa Show Supplier Material materials with Módulo elástico of 2.1 GPa | ASTM D 638 | 50 mm/min |
Resistencia a la flexión | 23.0 °C | 82 MPa Show Supplier Material materials with Resistencia a la flexión of 82 MPa | ASTM D 790 |
Resistencia a la tracción | 23.0 °C | 46 MPa Show Supplier Material materials with Resistencia a la tracción of 46 MPa | ASTM D 638 | break |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 150 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 150 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.1E-4 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.1E-4 1/K | ASTM D 696 | -30°C to 30°C |
Conductividad térmica | 23.0 °C | 2.8 W/(m·K) Show Supplier Material materials with Conductividad térmica of 2.8 W/(m·K) | ASTM E 1530 | |
Heat deflection temperature, 1.80 MPa | 73 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 73 °C | ASTM D 648 | 3.2mm, unannealed | |
Temperatura de flexión bajo carga | 73 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 73 °C |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 10 - 1000000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 10 - 1000000 Ω | ASTM D 257 |
Technological properties
Property | ||
---|---|---|
Application areas | Enclosures | |
Availability | Asia,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |