General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad relativa | 23.0 °C | 1.35 [-] Show Supplier Material materials with Densidad relativa of 1.35 [-] | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 3 % Show Supplier Material materials with Elongación of 3 % | ASTM D 638 | yld, Type I, 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 69 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 69 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 534 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 534 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 10 J Show Supplier Material materials with Instrumented Impact, Total Energy of 10 J | ASTM D 3763 | 23°C |
Módulo de flexión | 23.0 °C | 5.2 GPa Show Supplier Material materials with Módulo de flexión of 5.2 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Módulo elástico | 23.0 °C | 5.2 GPa Show Supplier Material materials with Módulo elástico of 5.2 GPa | ASTM D 638 | 5 mm/min |
Resistencia a la flexión | 23.0 °C | 193 MPa Show Supplier Material materials with Resistencia a la flexión of 193 MPa | ASTM D 790 | brk, 2.6 mm/min, 100 mm span |
Resistencia a la tracción | 23.0 °C | 119 MPa Show Supplier Material materials with Resistencia a la tracción of 119 MPa | ASTM D 638 | yld, Type I, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 69 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 69 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 3.6E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 3.6E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 8.1E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 8.1E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Heat deflection temperature, 0.45 MPa | 212 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 212 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Heat deflection temperature, 1.80 MPa | 205 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 205 °C | ASTM D 648 | 3.2mm, unannealed | |||
Relative temperature index, electrical | 155 °C Show Supplier Material materials with Relative temperature index, electrical of 155 °C | UL 746B | |||
Relative temperature index, mechanical impact | 155 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 155 °C | UL 746B | |||
Relative temperature index, mechanical strength | 155 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 155 °C | UL 746B | |||
Temperatura de flexión bajo carga | 205 - 212 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 205 - 212 °C | ||||
Temperatura de reblandecimiento Vicat | 210 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 210 °C | ASTM D 1525 | Rate B/50 | |||
Inflamabilidad | UL Recognized, 94V-0 Flame Class Rating: ≥0.4mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221094- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 0.4 mm Show Supplier Material materials with High Amp Arc Ignition of 0.4 mm | ≥, UL 746A | PLC 3 |
High Volt Arc Track Rate | 23.0 °C | 3 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 3 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 3 mm Show Supplier Material materials with Hot-Wire Ignition of 3 mm | ≥, UL 746A | PLC 1 |
Índice de seguimiento comparativo | 23.0 °C | 4 V Show Supplier Material materials with Índice de seguimiento comparativo of 4 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.7 % Show Supplier Material materials with Contracción of 0.7 % | SABIC method | 3.2 mm |
Contracción transversal | 23.0 °C | 0.6 % Show Supplier Material materials with Contracción transversal of 0.6 % | SABIC method | 3.2 mm |
Velocidad de flujo de la masa derretida | 19 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 19 g/10min | ASTM D 1238 | 337°C/6.6 kgf |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Data Management, Data Transfer, Wireless Communications, LED Lighting | |
Availability | Asia,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |