General
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 7 % Show Supplier Material materials with Elongación of 7 % | ASTM D 638 | yld, Type I, 5 mm/min |
Módulo de flexión | 23.0 °C | 3.5 GPa Show Supplier Material materials with Módulo de flexión of 3.5 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Módulo elástico | 23.0 °C | 3.6 GPa Show Supplier Material materials with Módulo elástico of 3.6 GPa | ASTM D 638 | 5 mm/min |
Resistencia a la flexión | 23.0 °C | 165 MPa Show Supplier Material materials with Resistencia a la flexión of 165 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Resistencia a la tracción | 23.0 °C | 110 MPa Show Supplier Material materials with Resistencia a la tracción of 110 MPa | ASTM D 638 | yld, Type I, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 32 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 32 kJ/m² | ASTM D 256 | notched, 23°C |
Taber Abrasion | 23.0 °C | 10 mg/1000cy Show Supplier Material materials with Taber Abrasion of 10 mg/1000cy | ASTM D 1044 | CS-17, 1 kg |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 5.58E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 5.58E-5 1/K | ASTM E 831 | -20°C to 150°C | ||
Conductividad térmica | 23.0 °C | 0.22 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.22 W/(m·K) | ASTM C177 | ||
Heat deflection temperature, 0.45 MPa | 207 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 207 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Heat deflection temperature, 1.80 MPa | 198 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 198 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Relative temperature index, electrical | 170 °C Show Supplier Material materials with Relative temperature index, electrical of 170 °C | UL 746B | |||
Relative temperature index, mechanical impact | 170 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 170 °C | UL 746B | |||
Relative temperature index, mechanical strength | 170 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 170 °C | UL 746B | |||
Temperatura de flexión bajo carga | 198 - 207 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 198 - 207 °C | ||||
Temperatura de reblandecimiento Vicat | 218 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 218 °C | ASTM D 1525 | Rate B/50 | |||
Inflamabilidad | NBS Smoke Density, Flaming, Ds 4 min: 2- ASTM E 662 <br> UL Recognized, 94-5VA Flame Class Rating: ≥3mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.75mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.4mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.4mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101048269- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Factor de disipación | 23.0 °C | 2.5E-3 [-] Show Supplier Material materials with Factor de disipación of 2.5E-3 [-] | ASTM D 150 | 2450 MHz |
High Amp Arc Ignition | 23.0 °C | 3 mm Show Supplier Material materials with High Amp Arc Ignition of 3 mm | ≥, UL 746A | PLC 3 |
High Volt Arc Track Rate | 23.0 °C | 2 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 2 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 0.75 mm Show Supplier Material materials with Hot-Wire Ignition of 0.75 mm | ≥, UL 746A | PLC 2 |
Rigidez dieléctrica | 23.0 °C | 32.7 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 32.7 kV/mm | ASTM D 149 | in air, 1.6 mm |
Volume resistivity | 23.0 °C | 1.00E+17 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+17 Ω·cm | ASTM D 257 |
Índice de seguimiento comparativo | 23.0 °C | 4 V Show Supplier Material materials with Índice de seguimiento comparativo of 4 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 % Show Supplier Material materials with Contracción of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Tray, Surgical Tray, Sunglasses, Wiring Devices, Wearables, Water Treatment/Filtration, Wireless Communications, Pipe/Fitting, Rear/Signal Lighting, Photo/Video Camera, Pharmaceutical Packaging & Drug Delivery, Power Manangement, Photovoltaic Components, Respiratory, Safety Glasses, Semiconductor, Security/Detection, Surgical Devices, Small Appliance, Smart/ID Card, Ignition System, Interior Rail Components, Meter Gas, Monitoring and Imaging, Medical Device, LED Lighting, Personal Computing, Oil/Gas, Personal Care, OLED, Lighting, Non-LED Lighting, Enclosure/Housing/Cover, Electronics, Enclosures, Electronic Components, Lab Ware and Clinical Diagnostics, Individual Equiptment, Industrial Material Handling, Fuel Cell, Gas/Electric Oven, Humidity Control, Eyeglasses, Front Grille, Forward Lighting, Food Processor, Food Container, Fog Lamp, Fluid Delivery, Exterior Rail Components, Electronic Material Handling, Engine Cooling System, Exterior Trim, Air Cabin Interiors, Aircraft Seating, Aerospace, Auto Electrical, Building Accessory, Circuit Protection, Audio, Auto Aftermarket, Composite, Commercial Storage/Cookware, Cooking Range, Coffee Maker/Espresso Machine, Data Transfer, Data Management, Displays, Dishwasher, Document Handling, Wire & cable, Adhesives | |
Availability | Europe,Asia,Americas | |
Processing methods | Front - Zone 3 Temperature: 345 to 400.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |