General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.19 g/cm³ Show Supplier Material materials with Densidad of 1.19 g/cm³ | ISO 1183 |
Densidad relativa | 23.0 °C | 1.19 [-] Show Supplier Material materials with Densidad relativa of 1.19 [-] | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 106 % Show Supplier Material materials with Elongación of 106 % | ISO 527 | break, 50 mm/min |
Hardness, Rockwell L | 23.0 °C | 83 [-] Show Supplier Material materials with Hardness, Rockwell L of 83 [-] | ASTM D 785 |
Hardness, Rockwell R | 23.0 °C | 117 [-] Show Supplier Material materials with Hardness, Rockwell R of 117 [-] | ASTM D 785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 660 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 660 J/m | ASTM D 256 |
Instrumented Impact, Total Energy | 23.0 °C | 67 J Show Supplier Material materials with Instrumented Impact, Total Energy of 67 J | ASTM D 3763 | 23°C |
Módulo de flexión | 23.0 °C | 2.2 GPa Show Supplier Material materials with Módulo de flexión of 2.2 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 2.1 GPa Show Supplier Material materials with Módulo elástico of 2.1 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 86 MPa Show Supplier Material materials with Resistencia a la flexión of 86 MPa | ISO 178 | yield, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 60 MPa Show Supplier Material materials with Resistencia a la tracción of 60 MPa | ISO 527 | break, 50 mm/min |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 29 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 29 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*3 sp=62mm, -30°C |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 46 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 46 kJ/m² | ISO 180/1A | notched 80*10*3, -30°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 7.42E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7.42E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 7.64E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 7.64E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Heat deflection temperature, 0.45 MPa | 131 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 131 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |||
Heat deflection temperature, 1.80 MPa | 117 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 117 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |||
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |||
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |||
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |||
Temperatura de flexión bajo carga | 117 - 131 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 117 - 131 °C | ||||
Temperatura de reblandecimiento Vicat | 138 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 138 °C | ISO 306 | Rate B/120 | |||
Inflamabilidad | UL Recognized, 94V-2 Flame Class Rating: ≥0.5mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.5mm UL 94 <br> UL Recognized, 94V-1 Flame Class Rating: ≥0.8mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥1.0mm UL 94 <br> UL Recognized, 94-5VA Flame Class Rating: ≥3.1mm UL 94 <br> UL Recognized, 94-5VB Flame Class Rating: ≥1.5mm UL 94 <br> Glow Wire Flammability Index 960°C, passes at: 1mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 1mm IEC 60695-2-12 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=102896543- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 1GHz | 23.0 °C | 2.78 [-] Show Supplier Material materials with Dielectric constant, 1GHz of 2.78 [-] | ASTM ES 7-83 | 1.1 GHz |
Dissipation factor, 1GHz | 23.0 °C | 6E-3 [-] Show Supplier Material materials with Dissipation factor, 1GHz of 6E-3 [-] | ASTM ES 7-83 | 1.1 GHz |
Sheet resistivity, ROA | 23.0 °C | 1.00E+16 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+16 Ω | >, ASTM D 257 |
Volume resistivity | 23.0 °C | 1.00E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+16 Ω·cm | >, ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.4 % Show Supplier Material materials with Contracción of 0.4 % | SABIC method | 3.2 mm |
Contracción transversal | 23.0 °C | 0.4 % Show Supplier Material materials with Contracción transversal of 0.4 % | SABIC method | 3.2 mm |
Velocidad de flujo de la masa derretida | 11.5 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 11.5 g/10min | ASTM D 1238 | 300°C/1.2 kgf | |
Velocidad de flujo del volumen derretido | 10 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 10 cm³/10min | ISO 1133 | MVR at 300°C/1.2 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Fast Charger, Mobile Phone, Drone, Battery Pack, Power Manangement, Scooter/Moped, Wireless Communications | |
Availability | Europe,Asia,Americas | |
Processing methods | Vent Depth: 0.025 to 0.076mm | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |