General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.47 g/cm³ Show Supplier Material materials with Densidad of 1.47 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 3.7 % Show Supplier Material materials with Elongación of 3.7 % | ISO 527 | break, 5 mm/min |
Módulo de flexión | 23.0 °C | 16.3 GPa Show Supplier Material materials with Módulo de flexión of 16.3 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 13.5 GPa Show Supplier Material materials with Módulo elástico of 13.5 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 267 MPa Show Supplier Material materials with Resistencia a la flexión of 267 MPa | ISO 178 | break, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 201 MPa Show Supplier Material materials with Resistencia a la tracción of 201 MPa | ISO 527 | break, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 9 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 9 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 35 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod no entallado of 35 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | UL 746B | |
Relative temperature index, mechanical impact | 130 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 130 °C | UL 746B | |
Relative temperature index, mechanical strength | 220 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 220 °C | UL 746B | |
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101284426- - <br> UL Recognized, 94V-0 Flame Class Rating: 0.7mm UL 94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 10 - 1000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 10 - 1000 Ω | ASTM D 257 |
Technological properties
Property | ||
---|---|---|
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120 to 150.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |