General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad relativa | 23.0 °C | 1.2 [-] Show Supplier Material materials with Densidad relativa of 1.2 [-] | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 120 % Show Supplier Material materials with Elongación of 120 % | ASTM D 638 | brk, Type I, 50 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 640 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 640 J/m | ASTM D 256 | notched, 23°C |
Instrumented Impact, at Peak | 23.0 °C | 54 J Show Supplier Material materials with Instrumented Impact, at Peak of 54 J | ASTM D 3763 | 23°C |
Módulo de flexión | 23.0 °C | 2.3 GPa Show Supplier Material materials with Módulo de flexión of 2.3 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Resistencia a la flexión | 23.0 °C | 93 MPa Show Supplier Material materials with Resistencia a la flexión of 93 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Resistencia a la tracción | 23.0 °C | 65 MPa Show Supplier Material materials with Resistencia a la tracción of 65 MPa | ASTM D 638 | brk, Type I, 50 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 640 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 640 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 126 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 126 °C | ASTM D 648 | 3.2mm, unannealed | |
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | UL 746B | |
Relative temperature index, mechanical impact | 130 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 130 °C | UL 746B | |
Relative temperature index, mechanical strength | 130 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C | UL 746B | |
Temperatura de flexión bajo carga | 126 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 126 °C | ||
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=103956751- - <br> UL Recognized, 94V-2 Flame Class Rating: ≥1.1mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥1.1mm UL 94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
High Volt Arc Track Rate | 23.0 °C | 2 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 2 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.1 mm Show Supplier Material materials with Hot-Wire Ignition of 1.1 mm | ≥, UL 746A | PLC 3 |
Índice de seguimiento comparativo | 23.0 °C | 2 V Show Supplier Material materials with Índice de seguimiento comparativo of 2 V | UL 746A | (UL) {PLC} |
Óptico
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 % Show Supplier Material materials with Contracción of 0.5 % | SABIC method | 3.2 mm |
Velocidad de flujo de la masa derretida | 25 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 25 g/10min | ASTM D 1238 | 300°C/1.2 kgf |
Technological properties
Property | ||
---|---|---|
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |