General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.22 % Show Supplier Material materials with Absorción de agua of 0.22 % | ISO 62-1 | (23°C/saturated) |
Densidad relativa | 23.0 °C | 1.25 [-] Show Supplier Material materials with Densidad relativa of 1.25 [-] | ASTM D 792 | |
Índice límite de óxigeno | 23.0 °C | 30 % Show Supplier Material materials with Índice límite de óxigeno of 30 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2 % Show Supplier Material materials with Elongación of 2 % | ISO 527 | break, 5 mm/min |
Módulo de flexión | 23.0 °C | 4.5 GPa Show Supplier Material materials with Módulo de flexión of 4.5 GPa | ISO 178 | 2 mm/min |
Resistencia a la flexión | 23.0 °C | 125 MPa Show Supplier Material materials with Resistencia a la flexión of 125 MPa | ISO 178 | break, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 80 MPa Show Supplier Material materials with Resistencia a la tracción of 80 MPa | ISO 527 | break, 5 mm/min |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 3E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 3E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Heat deflection temperature, 0.45 MPa | 135 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 135 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |||
Heat deflection temperature, 1.80 MPa | 130 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 130 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm | |||
Relative temperature index, electrical | 110 °C Show Supplier Material materials with Relative temperature index, electrical of 110 °C | UL 746B | |||
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |||
Relative temperature index, mechanical strength | 110 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 110 °C | UL 746B | |||
Temperatura de flexión bajo carga | 130 - 135 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 130 - 135 °C | ||||
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=104212941- - <br> UL Recognized, 94-5VA Flame Class Rating: ≥2mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥6mm UL 94 <br> UL Recognized, 94V-1 Flame Class Rating: ≥1.5mm UL 94 <br> Glow Wire Flammability Index, 1.0 mm: 960°C IEC 60695-2-12 <br> Glow Wire Ignitability Temperature, 1.0 mm: 800°C IEC 60695-2-13 <br> UV-light, water exposure/immersion: F2- UL 746C |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 60Hz | 23.0 °C | 3 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 3 [-] | IEC 60250 | 50/60 Hz |
Dissipation factor, 50Hz | 23.0 °C | 4E-3 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 4E-3 [-] | IEC 60250 | 50/60 Hz |
High Amp Arc Ignition | 23.0 °C | 1 mm Show Supplier Material materials with High Amp Arc Ignition of 1 mm | UL 746A | surface {PLC} |
High Volt Arc Track Rate | 23.0 °C | 4 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 0 mm Show Supplier Material materials with Hot-Wire Ignition of 0 mm | UL 746A | (PLC) |
Rigidez dieléctrica | 23.0 °C | 30 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 30 kV/mm | IEC 60243-1 | in oil, 0.8 mm |
Índice de seguimiento comparativo | 23.0 °C | 3 V Show Supplier Material materials with Índice de seguimiento comparativo of 3 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.2 % Show Supplier Material materials with Contracción of 0.2 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Enclosure/Housing/Cover, Energy Management, Electronics, Enclosures, Electronic Components, EV Infrastructure, Electronic Material Handling, EV/HEV Battery, Fixture Bath/Shower, Industrial Material Handling, Individual Equiptment, Hygiene/Personal Care, HVAC Underhood, Lab Ware and Clinical Diagnostics, Hot Water System, Humidity Control, Heavy Vehicles, Cluster, Coffee Maker/Espresso Machine, Battery System, Building Element, Data Transfer, Document Handling, Displays, Dishwasher, Defense Vehicles, Drain Pan, Air Conditioning, Battery Pack, Building Accessory, Circuit Protection, Audio, Auto Aftermarket, ATM/Ticket Machine, Security/Detection, Respiratory, Sensor, Surgical Devices, Pump, Pipe/Fitting, Power Manangement, Plumbing, Photovoltaic Components, Ignition System, Meter Gas, Microwave Oven, Personal Computing, Non-LED Lighting, Motorcycle, Wearables, Water Treatment/Filtration, Wiring Devices, Wireless Communications, Washing Machine, Travel Suitcase, Swimming Pool/Spa, Traffic Management | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 100 to 120.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |