NORYL™ Resin N1050 - Americas

Want to keep this datasheet? Save it now in your required format

Description

NORYL™ N1050 resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade was designed for improved dimensional stability and flow. This grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of 5VA at 2.5mm and V0 at 1.5mm along with impact strength, very low moisture absorption, excellent dimensional stability, and good electrical properties. NORYL N1050 resin is an excellent candidate for a variety of applications requiring electrically insulating properties, low moisture absorption and low warpage.

Los datos sobre este material han sido proporcionados por Sabic.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

Propiedades

General

PropertyTemperatureValueComment

Absorción de agua

23.0 °C

0.07 %

Show Supplier Material materials with Absorción de agua of 0.07 %

ASTM D 570 | (23°C/24hrs)

Densidad relativa

23.0 °C

1.1 [-]

Show Supplier Material materials with Densidad relativa of 1.1 [-]

ASTM D 792 |

Mecánica

PropertyTemperatureValueComment

Elongación

23.0 °C

40 %

Show Supplier Material materials with Elongación of 40 %

SABIC - Japan Method | break

Impact strength, Izod notched, ASTM

23.0 °C

117 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 117 J/m

ASTM D 256 | notched, 23°C

Módulo de flexión

23.0 °C

2.5 GPa

Show Supplier Material materials with Módulo de flexión of 2.5 GPa

ASTM D 790

Resistencia a la flexión

23.0 °C

98 MPa

Show Supplier Material materials with Resistencia a la flexión of 98 MPa

ASTM D 790

Resistencia a la tracción

23.0 °C

63 MPa

Show Supplier Material materials with Resistencia a la tracción of 63 MPa

SABIC - Japan Method | yield

Resistencia al choque, ensayo Izod entallado

23.0 °C

117 kJ/m²

Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 117 kJ/m²

ASTM D 256 | notched, 23°C

Aplicaciones térmicas

PropertyTemperatureValueComment

Coeficiente de dilatación térmica

23.0 °C

7E-5 1/K

Show Supplier Material materials with Coeficiente de dilatación térmica of 7E-5 1/K

TMA | -30°C to 30°C

Heat deflection temperature, 1.80 MPa

105 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 105 °C

ASTM D 648 | 6.4 mm, unannealed

Temperatura de flexión bajo carga

105 °C

Show Supplier Material materials with Temperatura de flexión bajo carga of 105 °C

Inflamabilidad

UL Recognized, 94V-0 Flame Class Rating: 1.5mm UL 94 <br> UL Recognized, 94-5VA Flame Class Rating: 2.5mm UL 94

Eléctrico

PropertyTemperatureValueComment

Dielectric constant, 60Hz

23.0 °C

2.78 [-]

Show Supplier Material materials with Dielectric constant, 60Hz of 2.78 [-]

ASTM D 150 | 50/60 Hz

Dissipation factor, 50Hz

23.0 °C

3E-3 [-]

Show Supplier Material materials with Dissipation factor, 50Hz of 3E-3 [-]

ASTM D 150 | 50/60 Hz

Sheet resistivity, ROA

23.0 °C

1.00E+16 Ω

Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+16 Ω

ASTM D 257

Rheological Properties

PropertyTemperatureValueComment

Contracción

23.0 °C

0.5 %

Show Supplier Material materials with Contracción of 0.5 %

SABIC method | 3.2 mm

Velocidad de flujo de la masa derretida

17 g/10min

Show Supplier Material materials with Velocidad de flujo de la masa derretida of 17 g/10min

ASTM D 1238 | 250°C/10.0 kgf

Technological properties

Property
Application areas

Photovoltaic Components, Power Manangement, Personal Computing, Washing Machine, Wireless Communications, Document Handling, Displays, Battery Cell, Battery Pack, Auto Electrical, EV Infrastructure, EV/HEV Battery, Enclosures, Energy Management, Enclosure/Housing/Cover, Electronic Components

Availability

Europe,Asia,Americas

Processing methods

Drying Temperature: 75 to 80.0°C
Drying Time: 3 to 4.0hrs
Drying Time (Cumulative): 8hrs
Maximum Moisture Content: 0.02%
Melt Temperature: 250 to 275.0°C
Nozzle Temperature: 250 to 275.0°C
Front - Zone 3 Temperature: 240 to 275.0°C
Middle - Zone 2 Temperature: 225 to 270.0°C
Rear - Zone 1 Temperature: 215 to 265.0°C
Mold Temperature: 55 to 75.0°C
Back Pressure: 0.3 to 0.7MPa
Screw Speed: 20 to 100.0rpm
Shot to Cylinder Size: 30 to 70.0%
Vent Depth: 0.038 to 0.051mm

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.