General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad relativa | 23.0 °C | 1.15 [-] Show Supplier Material materials with Densidad relativa of 1.15 [-] | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 3 % Show Supplier Material materials with Elongación of 3 % | ASTM D 638 | brk, Type I, 5 mm/min |
Hardness, Rockwell R | 23.0 °C | 122 [-] Show Supplier Material materials with Hardness, Rockwell R of 122 [-] | ASTM D 785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 69 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 69 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 240 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 240 J/m | ASTM D 4812 | 23°C |
Módulo de flexión | 23.0 °C | 6.9 GPa Show Supplier Material materials with Módulo de flexión of 6.9 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Resistencia a la flexión | 23.0 °C | 103 MPa Show Supplier Material materials with Resistencia a la flexión of 103 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Resistencia a la tracción | 23.0 °C | 71 MPa Show Supplier Material materials with Resistencia a la tracción of 71 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 69 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 69 kJ/m² | ASTM D 256 | notched, 23°C |
Taber Abrasion | 23.0 °C | 83 mg/1000cy Show Supplier Material materials with Taber Abrasion of 83 mg/1000cy | ASTM D 1044 | CS-17, 1 kg |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 111 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 111 °C | ASTM D 648 | 6.4 mm, unannealed | |
Heat deflection temperature, 1.80 MPa | 105 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 105 °C | ASTM D 648 | 6.4 mm, unannealed | |
Temperatura de flexión bajo carga | 105 - 111 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 105 - 111 °C | ||
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=221166- - <br> UL Recognized, 94V-1 Flame Class Rating: 2mm UL 94 <br> UL Recognized, 94-5VA Flame Class Rating: 2mm UL 94 |
Eléctrico
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Electrical Components & Infrastructure | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 90 to 95.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |