General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.1 % Show Supplier Material materials with Absorción de agua of 0.1 % | ISO 62-1 | (23°C/24hrs) |
Coefficient of friction | 0.48 - 0.64 [-] Show Supplier Material materials with Coefficient of friction of 0.48 - 0.64 [-] | ||
Coefficient of friction, kinetic | 0.48 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.48 [-] | ASTM D 3702 Modified: Manual | |
Coefficient of friction, static | 0.64 [-] Show Supplier Material materials with Coefficient of friction, static of 0.64 [-] | ASTM D 3702 Modified: Manual | |
Densidad | 23.0 °C | 1.45 g/cm³ Show Supplier Material materials with Densidad of 1.45 g/cm³ | ISO 1183 |
Densidad relativa | 23.0 °C | 1.45 [-] Show Supplier Material materials with Densidad relativa of 1.45 [-] | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.1 % Show Supplier Material materials with Moisture absorption of 0.1 % | ISO 62 | (23°C / 50% RH) |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2.8 % Show Supplier Material materials with Elongación of 2.8 % | ISO 527 | break, 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 150 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 150 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 700 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 700 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, at Peak | 23.0 °C | 22 J Show Supplier Material materials with Instrumented Impact, at Peak of 22 J | ASTM D 3763 | 23°C |
Módulo de flexión | 23.0 °C | 6 GPa Show Supplier Material materials with Módulo de flexión of 6 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 6.6 GPa Show Supplier Material materials with Módulo elástico of 6.6 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 150 MPa Show Supplier Material materials with Resistencia a la flexión of 150 MPa | ISO 178 | 2 mm/min |
Resistencia a la tracción | 23.0 °C | 97 MPa Show Supplier Material materials with Resistencia a la tracción of 97 MPa | ISO 527 | break, 5 mm/min |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 21 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 21 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*4 sp=62mm, 23°C |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 15 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 15 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 49 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod no entallado of 49 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 2.5E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.5E-5 1/K | ISO 11359-2 | 23°C to 60°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 7.8E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 7.8E-5 1/K | ISO 11359-2 | 23°C to 60°C | ||
Heat deflection temperature, 0.45 MPa | 146 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 146 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 142 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 142 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |||
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |||
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |||
Temperatura de flexión bajo carga | 142 - 146 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 142 - 146 °C | ||||
Temperatura de reblandecimiento Vicat | 148 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 148 °C | ISO 306 | Rate B/50 | |||
Inflamabilidad | UL Recognized, 94V-1 Flame Class Rating: ≥3mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101344537- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=101344452- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 3 mm Show Supplier Material materials with High Amp Arc Ignition of 3 mm | ≥, UL 746A | PLC 2 |
Hot-Wire Ignition | 23.0 °C | 3 mm Show Supplier Material materials with Hot-Wire Ignition of 3 mm | ≥, UL 746A | PLC 0 |
Índice de seguimiento comparativo | 23.0 °C | 3 V Show Supplier Material materials with Índice de seguimiento comparativo of 3 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.2 % Show Supplier Material materials with Contracción of 0.2 % | SABIC method |
Contracción transversal | 23.0 °C | 0.3 % Show Supplier Material materials with Contracción transversal of 0.3 % | SABIC method |
Velocidad de flujo de la masa derretida | 8.8 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 8.8 g/10min | ASTM D 1238 | 300°C/2.16 kgf | |
Velocidad de flujo del volumen derretido | 5 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 5 cm³/10min | ISO 1133 | MVR at 300°C/2.16 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Air Cabin Interiors, Circuit Protection, Document Handling, Electronic Components, Surgical Devices, Renal and Blood Handling, Medical Device, Wearables, Wiring Devices | |
Availability | Europe,Asia,Americas | |
Processing methods | Back Pressure: 0.2 to 0.3MPa | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |