General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.5 % Show Supplier Material materials with Absorción de agua of 0.5 % | ISO 62-1 | (23°C/saturated) |
Densidad | 23.0 °C | 1.44 g/cm³ Show Supplier Material materials with Densidad of 1.44 g/cm³ | ASTM D 792 |
Densidad relativa | 23.0 °C | 1.44 [-] Show Supplier Material materials with Densidad relativa of 1.44 [-] | ASTM D 792 | |
Moisture absorption | 23.0 °C | 0.15 % Show Supplier Material materials with Moisture absorption of 0.15 % | ISO 62 | (23°C / 50% RH) |
Specific volume | 23.0 °C | 0.7 cm³/g Show Supplier Material materials with Specific volume of 0.7 cm³/g | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 3 % Show Supplier Material materials with Elongación of 3 % | ISO 527 | yield, 5 mm/min |
Hardness, Rockwell R | 23.0 °C | 109 [-] Show Supplier Material materials with Hardness, Rockwell R of 109 [-] | ASTM D 785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 112 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 112 J/m | ASTM D 256 | notched, -30°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 640 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 640 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 17 J Show Supplier Material materials with Instrumented Impact, Total Energy of 17 J | ASTM D 3763 | 23°C |
Instrumented Impact, at Peak | 23.0 °C | 5 J Show Supplier Material materials with Instrumented Impact, at Peak of 5 J | ASTM D 3763 | 23°C |
Módulo de flexión | 23.0 °C | 7.8 GPa Show Supplier Material materials with Módulo de flexión of 7.8 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 8.5 GPa Show Supplier Material materials with Módulo elástico of 8.5 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 154 MPa Show Supplier Material materials with Resistencia a la flexión of 154 MPa | ISO 178 | yield, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 105 MPa Show Supplier Material materials with Resistencia a la tracción of 105 MPa | ISO 527 | yield, 5 mm/min |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 9 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 9 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*3 sp=62mm, 23°C |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 6 kJ/m² | ISO 180/1A | notched 80*10*4, -30°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 2.7E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.7E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 1.1E-4 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 1.1E-4 1/K | ISO 11359-2 | -40°C to 40°C | ||
Heat deflection temperature, 0.45 MPa | 204 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 204 °C | ASTM D 648 | 6.4 mm, unannealed | |||
Heat deflection temperature, 1.80 MPa | 155 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 155 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 140 °C Show Supplier Material materials with Relative temperature index, electrical of 140 °C | UL 746B | |||
Relative temperature index, mechanical impact | 130 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 130 °C | UL 746B | |||
Relative temperature index, mechanical strength | 140 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 140 °C | UL 746B | |||
Temperatura de flexión bajo carga | 155 - 204 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 155 - 204 °C | ||||
Temperatura de reblandecimiento Vicat | 150 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 150 °C | ISO 306 | Rate B/120 | |||
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=103956403- - <br> UL Recognized, 94HB Flame Class Rating: ≥1.5mm UL 94 <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=103938404- - |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica, 1 MHz | 23.0 °C | 4 [-] Show Supplier Material materials with Constante dieléctrica, 1 MHz of 4 [-] | ASTM D 150 |
Constante dieléctrica, 100 Hz | 23.0 °C | 4 [-] Show Supplier Material materials with Constante dieléctrica, 100 Hz of 4 [-] | ASTM D 150 |
Dissipation factor, 100Hz | 23.0 °C | 3E-3 [-] Show Supplier Material materials with Dissipation factor, 100Hz of 3E-3 [-] | ASTM D 150 |
Dissipation factor, 1MHz | 23.0 °C | 0.02 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 0.02 [-] | ASTM D 150 | |
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 3 |
High Volt Arc Track Rate | 23.0 °C | 1 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 1 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 2 |
Rigidez dieléctrica | 23.0 °C | 27 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 27 kV/mm | IEC 60243-1 | in oil, 1.6 mm |
Volume resistivity | 23.0 °C | 4.80E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 4.80E+15 Ω·cm | ASTM D 257 |
Índice de seguimiento comparativo | 23.0 °C | 2 V Show Supplier Material materials with Índice de seguimiento comparativo of 2 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.3 % Show Supplier Material materials with Contracción of 0.3 % | SABIC method | 0.75-2.3 mm |
Contracción transversal | 23.0 °C | 0.7 % Show Supplier Material materials with Contracción transversal of 0.7 % | SABIC method | 2.3-4.6 mm |
Velocidad de flujo de la masa derretida | 24 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 24 g/10min | ASTM D 1238 | 250°C/5.0 kgf | |
Velocidad de flujo del volumen derretido | 19 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 19 cm³/10min | ISO 1133 | MVR at 265°C/5.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 110°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |