General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.35 % Show Supplier Material materials with Absorción de agua of 0.35 % | ISO 62-1 | (23°C/saturated) |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 220 % Show Supplier Material materials with Elongación of 220 % | SABIC - Japan Method | break |
Módulo de flexión | 23.0 °C | 2.3 GPa Show Supplier Material materials with Módulo de flexión of 2.3 GPa | ISO 178 | 2 mm/min |
Resistencia a la flexión | 23.0 °C | 90 MPa Show Supplier Material materials with Resistencia a la flexión of 90 MPa | ISO 178 | yield, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 61 MPa Show Supplier Material materials with Resistencia a la tracción of 61 MPa | SABIC - Japan Method | yield |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 65 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 65 kJ/m² | ISO 180/1A | 80*10*3, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 7E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7E-5 1/K | TMA | -30°C to 30°C |
Heat deflection temperature, 0.45 MPa | 133 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 133 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm | |
Temperatura de flexión bajo carga | 133 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 133 °C |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 % Show Supplier Material materials with Contracción of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Audio, Auto Aftermarket, Data Transfer, Data Management, Cluster, Console, Displays, Doors Hardware/Trim, Forward Lighting, Heavy Vehicles, Infotainment/Telematic, Electronic Components, Power Manangement, Rear/Signal Lighting, Small Appliance, Surgical Devices, Non-LED Lighting, Personal Computing, Meter Gas, LED Lighting, Wireless Communications, Trim | |
Availability | Europe,Asia | |
Processing methods | Front - Zone 3 Temperature: 280 to 300.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |