General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.45 g/cm³ Show Supplier Material materials with Densidad of 1.45 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.2 % Show Supplier Material materials with Moisture absorption of 0.2 % | ASTM D 570 | (23°C/50% RH/24 hrs) |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 1.9 % Show Supplier Material materials with Elongación of 1.9 % | ISO 527 | break, 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 64 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 64 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 662 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 662 J/m | ASTM D 4812 | 23°C |
Módulo de flexión | 23.0 °C | 9.1 GPa Show Supplier Material materials with Módulo de flexión of 9.1 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 11.3 GPa Show Supplier Material materials with Módulo elástico of 11.3 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 189 MPa Show Supplier Material materials with Resistencia a la flexión of 189 MPa | ISO 178 |
Resistencia a la tracción | 23.0 °C | 128 MPa Show Supplier Material materials with Resistencia a la tracción of 128 MPa | ISO 527 | break, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 5 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 32 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod no entallado of 32 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 2.5E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.5E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 5.11E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 5.11E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Heat deflection temperature, 0.45 MPa | 299 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 299 °C | ASTM D 648 | 3.2 mm, unannealed | |||
Heat deflection temperature, 1.80 MPa | 277 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 277 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 125 °C Show Supplier Material materials with Relative temperature index, electrical of 125 °C | UL 746B | |||
Relative temperature index, mechanical impact | 50 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 50 °C | UL 746B | |||
Relative temperature index, mechanical strength | 125 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 125 °C | UL 746B | |||
Temperatura de flexión bajo carga | 277 - 299 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 277 - 299 °C | ||||
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101284114- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=103093678- - <br> UL Recognized, 94V-0 Flame Class Rating: ≥1.5mm UL 94 <br> UL Recognized, 94V-1 Flame Class Rating: ≥1mm UL 94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica, 1 MHz | 23.0 °C | 3.82 [-] Show Supplier Material materials with Constante dieléctrica, 1 MHz of 3.82 [-] | ASTM D 150 |
Dissipation factor, 1MHz | 23.0 °C | 0.01 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 0.01 [-] | ASTM D 150 | |
Dissipation factor, 1kHz | 23.0 °C | 0.01 [-] Show Supplier Material materials with Dissipation factor, 1kHz of 0.01 [-] | ASTM D 150 |
High Volt Arc Track Rate | 23.0 °C | 2 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 2 PLC Code | UL 746A | (PLC) |
Rigidez dieléctrica | 23.0 °C | 29.7 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 29.7 kV/mm | ASTM D 149 | in oil, 0.8 mm |
Índice de seguimiento comparativo | 23.0 °C | 0 V Show Supplier Material materials with Índice de seguimiento comparativo of 0 V | UL 746A | (UL) {PLC} |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Data Transfer | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 90 to 110.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |