LNP THERMOCOMP* AF002XXC is a compound based on ABS resin containing 10% Glass Fiber.

Los datos sobre este material han sido proporcionados por Sabic.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValueComment

Densidad

23.0 °C

1.1 g/cm³

Show Supplier Material materials with Densidad of 1.1 g/cm³

ISO 1183

Moisture absorption

23.0 °C

0.38 %

Show Supplier Material materials with Moisture absorption of 0.38 %

ISO 62 | (23°C / 50% RH)

Mecánica

PropertyTemperatureValueComment

Elongación

23.0 °C

2.7 %

Show Supplier Material materials with Elongación of 2.7 %

ISO 527 | break

Impact strength, Izod notched, ASTM

23.0 °C

80 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 80 J/m

ASTM D 256

Impact strength, Izod unnotched, ASTM

23.0 °C

320 J/m

Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 320 J/m

ASTM D 4812 | 23°C

Instrumented Impact, at Peak

23.0 °C

15 J

Show Supplier Material materials with Instrumented Impact, at Peak of 15 J

ASTM D 3763 | 23°C

Módulo de flexión

23.0 °C

4.5 GPa

Show Supplier Material materials with Módulo de flexión of 4.5 GPa

ISO 178

Módulo elástico

23.0 °C

4.2 GPa

Show Supplier Material materials with Módulo elástico of 4.2 GPa

ISO 527 | 1 mm/min

Resistencia a la flexión

23.0 °C

107 MPa

Show Supplier Material materials with Resistencia a la flexión of 107 MPa

ISO 178

Resistencia a la tracción

23.0 °C

64 MPa

Show Supplier Material materials with Resistencia a la tracción of 64 MPa

ISO 527 | break

Resistencia al choque, ensayo Izod entallado

23.0 °C

9 kJ/m²

Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 9 kJ/m²

ISO 180/1A | notched 80*10*4, 23°C

Resistencia al choque, ensayo Izod no entallado

23.0 °C

24 kJ/m²

Show Supplier Material materials with Resistencia al choque, ensayo Izod no entallado of 24 kJ/m²

ISO 180/1U | 80*10*4, 23°C

Aplicaciones térmicas

PropertyValueComment

Heat deflection temperature, 0.45 MPa

101 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 101 °C

ASTM D 648 | 3.2 mm, unannealed

Heat deflection temperature, 1.80 MPa

95 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 95 °C

ISO 75/Af | Flatw 80*10*4 sp=64mm

Relative temperature index, electrical

60 °C

Show Supplier Material materials with Relative temperature index, electrical of 60 °C

UL 746B

Relative temperature index, mechanical impact

60 °C

Show Supplier Material materials with Relative temperature index, mechanical impact of 60 °C

UL 746B

Relative temperature index, mechanical strength

60 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 60 °C

UL 746B

Temperatura de flexión bajo carga

95 - 101 °C

Show Supplier Material materials with Temperatura de flexión bajo carga of 95 - 101 °C

Inflamabilidad

UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101344528- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=101343852- - <br> UL Recognized, 94HB Flame Class Rating: 1.5mm UL 94

Rheological Properties

PropertyTemperatureValueComment

Contracción

23.0 °C

0.41 %

Show Supplier Material materials with Contracción of 0.41 %

ISO 294 | 24 hrs

Contracción transversal

23.0 °C

0.38 %

Show Supplier Material materials with Contracción transversal of 0.38 %

ISO 294 | 24 hrs

Technological properties

Property
Application areas

Lab Ware and Clinical Diagnostics, Document Handling

Availability

Europe,Asia,Americas

Processing methods

Drying Temperature: 80°C
Drying Time: 4hrs
Maximum Moisture Content: 0.05 to 0.1%
Melt Temperature: 260°C
Front - Zone 3 Temperature: 265 to 275.0°C
Middle - Zone 2 Temperature: 230 to 245.0°C
Rear - Zone 1 Temperature: 205 to 215.0°C
Mold Temperature: 70 to 80.0°C
Back Pressure: 0.2 to 0.3MPa
Screw Speed: 30 to 60.0rpm

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.