General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.8 g/cm³ Show Supplier Material materials with Densidad of 1.8 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2 % Show Supplier Material materials with Elongación of 2 % | ISO 527 | break, 5 mm/min |
Módulo de flexión | 23.0 °C | 12.7 GPa Show Supplier Material materials with Módulo de flexión of 12.7 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 14.7 GPa Show Supplier Material materials with Módulo elástico of 14.7 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 206 MPa Show Supplier Material materials with Resistencia a la flexión of 206 MPa | ISO 178 | yield, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 147 MPa Show Supplier Material materials with Resistencia a la tracción of 147 MPa | ISO 527 | break, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 7 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 30 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod no entallado of 30 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.6E-5 1/K | ISO 11359-2 | 23°C to 60°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 3.8E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 3.8E-5 1/K | ISO 11359-2 | 23°C to 60°C | ||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||||
Glow Wire Ignition Temperature | 875 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 875 °C | IEC 60695-2-13 | 2.0 mm | |||
Heat deflection temperature, 0.45 MPa | 280 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 280 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 264 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 264 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | UL 746B | |||
Relative temperature index, mechanical impact | 130 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 130 °C | UL 746B | |||
Relative temperature index, mechanical strength | 130 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C | UL 746B | |||
Temperatura de flexión bajo carga | 264 - 280 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 264 - 280 °C | ||||
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101658602- - <br> UL Recognized, 94V-0 Flame Class Rating: ≥1.7mm UL 94 <br> Glow Wire Ignitability Temperature, 1.0 mm: 825°C IEC 60695-2-13 <br> Glow Wire Flammability Index, 1.0 mm: 960°C IEC 60695-2-12 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Índice de seguimiento comparativo | 23.0 °C | 175 V Show Supplier Material materials with Índice de seguimiento comparativo of 175 V | IEC 60112 | |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.2 % Show Supplier Material materials with Contracción of 0.2 % | SABIC method |
Technological properties
Property | ||
---|---|---|
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120 to 150.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |