General
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.61 [-] Show Supplier Material materials with Coefficient of friction of 0.61 [-] | ||
Coefficient of friction, kinetic | 0.61 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.61 [-] | ASTM D 3702 Modified: Manual | |
Densidad | 23.0 °C | 1.46 g/cm³ Show Supplier Material materials with Densidad of 1.46 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 3.3 % Show Supplier Material materials with Elongación of 3.3 % | ASTM D 638 | break |
Resistencia a la flexión | 23.0 °C | 262 MPa Show Supplier Material materials with Resistencia a la flexión of 262 MPa | ISO 178 |
Resistencia a la tracción | 23.0 °C | 185 MPa Show Supplier Material materials with Resistencia a la tracción of 185 MPa | ASTM D 638 | break |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 3E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 3E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | UL 746B | |||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | UL 746B | |||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | UL 746B | |||
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101282712- - <br> UL Recognized, 94HB Flame Class Rating: ≥1.5mm UL 94 |
Technological properties
Property | ||
---|---|---|
Application areas | Wireless Communications, Document Handling | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |