General
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.57 - 0.71 [-] Show Supplier Material materials with Coefficient of friction of 0.57 - 0.71 [-] | ||
Coefficient of friction, kinetic | 0.71 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.71 [-] | ASTM D 3702 Modified: Manual | |
Coefficient of friction, static | 0.57 [-] Show Supplier Material materials with Coefficient of friction, static of 0.57 [-] | ASTM D 3702 Modified: Manual | |
Densidad | 23.0 °C | 1.39 g/cm³ Show Supplier Material materials with Densidad of 1.39 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 1.2 % Show Supplier Material materials with Moisture absorption of 1.2 % | ISO 62 | (23°C / 50% RH) |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Impact strength, Izod notched, ASTM | 23.0 °C | 58 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 58 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 646 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 646 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, at Peak | 23.0 °C | 6 J Show Supplier Material materials with Instrumented Impact, at Peak of 6 J | ASTM D 3763 | 23°C |
Módulo de flexión | 23.0 °C | 9.4 GPa Show Supplier Material materials with Módulo de flexión of 9.4 GPa | ASTM D 790 |
Módulo elástico | 23.0 °C | 9 GPa Show Supplier Material materials with Módulo elástico of 9 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 235 MPa Show Supplier Material materials with Resistencia a la flexión of 235 MPa | ASTM D 790 |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 7 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 52 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod no entallado of 52 kJ/m² | ISO 180/1U | unnotched 80*10*4 |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 3.04E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 3.04E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 7.32E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 7.32E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Heat deflection temperature, 0.45 MPa | 265 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 265 °C | ASTM D 648 | 3.2 mm, unannealed | |||
Heat deflection temperature, 1.80 MPa | 243 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 243 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | UL 746B | |||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | UL 746B | |||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | UL 746B | |||
Temperatura de flexión bajo carga | 243 - 265 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 243 - 265 °C | ||||
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101282588- - <br> UL Recognized, 94HB Flame Class Rating: 1.5mm UL 94 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Fluid Delivery | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |