Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2.7 % Show Supplier Material materials with Elongación of 2.7 % | ASTM D 638 | break |
Impact strength, Izod notched, ASTM | 23.0 °C | 64 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 64 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 534 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 534 J/m | ASTM D 4812 | 23°C |
Módulo de flexión | 23.0 °C | 7.6 GPa Show Supplier Material materials with Módulo de flexión of 7.6 GPa | ASTM D 790 |
Módulo elástico | 23.0 °C | 8.3 GPa Show Supplier Material materials with Módulo elástico of 8.3 GPa | ASTM D 638 | 50 mm/min |
Resistencia a la flexión | 23.0 °C | 179 MPa Show Supplier Material materials with Resistencia a la flexión of 179 MPa | ASTM D 790 |
Resistencia a la tracción | 23.0 °C | 110 MPa Show Supplier Material materials with Resistencia a la tracción of 110 MPa | ASTM D 638 | break |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 64 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 64 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 141 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 141 °C | ASTM D 648 | 3.2mm, unannealed | |
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |
Temperatura de flexión bajo carga | 141 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 141 °C | ||
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101345261- - <br> UL Recognized, 94-5VA Flame Class Rating: ≥3mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥1.5mm UL 94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 10 - 1000000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 10 - 1000000 Ω | ASTM D 257 |
Technological properties
Property | ||
---|---|---|
Application areas | ATM/Ticket Machine | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |