General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.37 g/cm³ Show Supplier Material materials with Densidad of 1.37 g/cm³ | ISO 1183 |
Densidad relativa | 23.0 °C | 1.35 [-] Show Supplier Material materials with Densidad relativa of 1.35 [-] | ASTM D 792 | |
Moisture absorption | 23.0 °C | 0.83 % Show Supplier Material materials with Moisture absorption of 0.83 % | ISO 62 | (23°C / 50% RH) |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 8.1 % Show Supplier Material materials with Elongación of 8.1 % | ASTM D 638 | brk, Type I, 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 106 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 106 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 727 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 727 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, at Peak | 23.0 °C | 16 J Show Supplier Material materials with Instrumented Impact, at Peak of 16 J | ASTM D 3763 | 23°C |
Módulo de flexión | 23.0 °C | 6.8 GPa Show Supplier Material materials with Módulo de flexión of 6.8 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Módulo elástico | 23.0 °C | 9.7 GPa Show Supplier Material materials with Módulo elástico of 9.7 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 157 MPa Show Supplier Material materials with Resistencia a la flexión of 157 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Resistencia a la tracción | 23.0 °C | 35 MPa Show Supplier Material materials with Resistencia a la tracción of 35 MPa | ISO 527 | yield, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 10 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 53 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod no entallado of 53 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 141 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 141 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |
Heat deflection temperature, 1.80 MPa | 135 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 135 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | UL 746B | |
Relative temperature index, mechanical impact | 70 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 70 °C | UL 746B | |
Relative temperature index, mechanical strength | 85 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 85 °C | UL 746B | |
Temperatura de flexión bajo carga | 135 - 141 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 135 - 141 °C | ||
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=103093413- - <br> UL Recognized, 94HB Flame Class Rating: ≥1.5mm UL 94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with High Amp Arc Ignition of 1.5 mm | ≥, UL 746A | PLC 0 |
High Volt Arc Track Rate | 23.0 °C | 1 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 1 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 3 mm Show Supplier Material materials with Hot-Wire Ignition of 3 mm | ≥, UL 746A | PLC 0 |
Índice de seguimiento comparativo | 23.0 °C | 0 V Show Supplier Material materials with Índice de seguimiento comparativo of 0 V | UL 746A | (UL) {PLC} |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |