General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.1 % Show Supplier Material materials with Absorción de agua of 0.1 % | ISO 62-1 | (23°C/24hrs) |
Coefficient of friction | 0.41 - 0.57 [-] Show Supplier Material materials with Coefficient of friction of 0.41 - 0.57 [-] | ||
Coefficient of friction, kinetic | 0.57 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.57 [-] | ASTM D 3702 Modified: Manual | |
Coefficient of friction, static | 0.41 [-] Show Supplier Material materials with Coefficient of friction, static of 0.41 [-] | ASTM D 3702 Modified: Manual | |
Densidad | 23.0 °C | 1.68 g/cm³ Show Supplier Material materials with Densidad of 1.68 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.05 % Show Supplier Material materials with Moisture absorption of 0.05 % | ISO 62 | (23°C / 50% RH) |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2.8 % Show Supplier Material materials with Elongación of 2.8 % | ISO 527 | break, 5 mm/min |
Flexural strain | 23.0 °C | 3.1 % Show Supplier Material materials with Flexural strain of 3.1 % | ISO 178 | break, 2 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 90 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 90 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 750 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 750 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, at Peak | 23.0 °C | 13 J Show Supplier Material materials with Instrumented Impact, at Peak of 13 J | ASTM D 3763 | 23°C |
Módulo de flexión | 23.0 °C | 8.9 GPa Show Supplier Material materials with Módulo de flexión of 8.9 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 10.1 GPa Show Supplier Material materials with Módulo elástico of 10.1 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 183 MPa Show Supplier Material materials with Resistencia a la flexión of 183 MPa | ISO 178 | yield, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 114 MPa Show Supplier Material materials with Resistencia a la tracción of 114 MPa | ISO 527 | break, 5 mm/min |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 9 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 9 kJ/m² | ISO 179/1eA | V-notch Edgew, 23°C, 80*10*4 sp=62mm |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 9 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 9 kJ/m² | ISO 180/1A | notched 80*10*3, -40°C |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 60 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod no entallado of 60 kJ/m² | ISO 180/1U | unnotched 80*10*4, -40°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Calor específico | 23.0 °C | 1751 J/(kg·K) Show Supplier Material materials with Calor específico of 1751 J/(kg·K) | ASTM E 1269 | ||
Coeficiente de dilatación térmica | 23.0 °C | 3.8E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 3.8E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 6.7E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 6.7E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Conductividad térmica | 23.0 °C | 0.26 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.26 W/(m·K) | ASTM D 5930 | ||
Heat deflection temperature, 0.45 MPa | 222 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 222 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 208 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 208 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 75 °C Show Supplier Material materials with Relative temperature index, electrical of 75 °C | UL 746B | |||
Relative temperature index, mechanical impact | 75 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 75 °C | UL 746B | |||
Relative temperature index, mechanical strength | 75 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 75 °C | UL 746B | |||
Temperatura de flexión bajo carga | 208 - 222 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 208 - 222 °C | ||||
Temperatura de reblandecimiento Vicat | 212 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 212 °C | ISO 306 | Rate B/50 | |||
Inflamabilidad | UL Recognized, 94HB Flame Class Rating: 1.5mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101282605- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=103093711- - <br> UL Yellow Card Link 3: https://iq.ul.com/ul/cert.aspx?ULID=101282616- - |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.1 % Show Supplier Material materials with Contracción of 0.1 % | SABIC method |
Contracción transversal | 23.0 °C | 0.5 % Show Supplier Material materials with Contracción transversal of 0.5 % | SABIC method |
Velocidad de flujo de la masa derretida | 22 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 22 g/10min | ASTM D 1238 | 250°C/5.0 kgf | |
Velocidad de flujo del volumen derretido | 17 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 17 cm³/10min | ISO 1133 | MVR at 250°C/5.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Commercial Appliance, Data Management, Data Transfer, Displays, Electronic Components, Electronics, Heavy Vehicles, Gear/Bearing/Slider, Engine Component, Medical Device, Oil/Gas, Personal Computing, Security/Detection, Pharmaceutical Packaging & Drug Delivery, Pallet | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |