General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.162 g/cm³ Show Supplier Material materials with Densidad of 1.162 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.5 % Show Supplier Material materials with Moisture absorption of 0.5 % | ASTM D 570 | (23°C/50% RH/24 hrs) |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 10 % Show Supplier Material materials with Elongación of 10 % | ASTM D 638 | brk, Type I, 5 mm/min |
Módulo de flexión | 23.0 °C | 4 GPa Show Supplier Material materials with Módulo de flexión of 4 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Resistencia a la flexión | 23.0 °C | 155 MPa Show Supplier Material materials with Resistencia a la flexión of 155 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Resistencia a la tracción | 23.0 °C | 89 MPa Show Supplier Material materials with Resistencia a la tracción of 89 MPa | ASTM D 638 | yld, Type I, 5 mm/min |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 3.9E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 3.9E-5 1/K | ASTM E 831 | -20°C to 150°C |
Temperatura de reblandecimiento Vicat | 240 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 240 °C | ASTM D 1525 | Rate B/50 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.6 % Show Supplier Material materials with Contracción of 0.6 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Application areas | Auto Electrical, Electronic Components, Enclosures, Enclosure/Housing/Cover, Exterior Trim, Forward Lighting, Fixture Bath/Shower, Fog Lamp, Lab Ware and Clinical Diagnostics, Lawn/Garden, Individual Equiptment, Recreational Vehicle, Power Boat, Pipe/Fitting, Rear/Signal Lighting, Photo/Video Camera, Plumbing, Wireless Communications | |
Availability | Europe,Asia,MEA,Americas | |
Processing methods | Rear - Zone 1 Temperature: 265 to 305.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |