General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad relativa | 23.0 °C | 1.21 [-] Show Supplier Material materials with Densidad relativa of 1.21 [-] | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Impact strength, Izod notched, ASTM | 23.0 °C | 694 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 694 J/m | ASTM D 256 | notched, 23°C |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 694 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 694 kJ/m² | ASTM D 256 | notched, 23°C |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 23.8 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 23.8 g/10min | ASTM D 1238 | 300°C/1.2 kgf |
Velocidad de flujo del volumen derretido | 23 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 23 cm³/10min | ISO 1133 | MVR at 300°C/1.2 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Surgical Devices | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |