General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.25 g/cm³ Show Supplier Material materials with Densidad of 1.25 g/cm³ | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 5.7 % Show Supplier Material materials with Elongación of 5.7 % | ASTM D 638 | brk, Type I, 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 160 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 160 J/m | ASTM D 256 | notched, 23°C |
Módulo de flexión | 23.0 °C | 3.4 GPa Show Supplier Material materials with Módulo de flexión of 3.4 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Resistencia a la flexión | 23.0 °C | 121 MPa Show Supplier Material materials with Resistencia a la flexión of 121 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Resistencia a la tracción | 23.0 °C | 74 MPa Show Supplier Material materials with Resistencia a la tracción of 74 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 160 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 160 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 127 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 127 °C | ASTM D 648 | 3.2mm, unannealed | |
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |
Temperatura de flexión bajo carga | 127 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 127 °C | ||
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=103722308- - <br> UL Recognized, 94HB Flame Class Rating: 0.8mm UL 94 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo del volumen derretido | 17 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 17 cm³/10min | ASTM D 1238 | MVR at 300°C/1.2 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Wireless Communications | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 110°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |