General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad relativa | 23.0 °C | 1.42 [-] Show Supplier Material materials with Densidad relativa of 1.42 [-] | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 2.7 % Show Supplier Material materials with Elongación of 2.7 % | ISO 527 | break, 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 196 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 196 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 752 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 752 J/m | ASTM D 4812 | 23°C |
Módulo de flexión | 23.0 °C | 7.7 GPa Show Supplier Material materials with Módulo de flexión of 7.7 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 8.3 GPa Show Supplier Material materials with Módulo elástico of 8.3 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 182 MPa Show Supplier Material materials with Resistencia a la flexión of 182 MPa | ISO 178 | yield, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 119 MPa Show Supplier Material materials with Resistencia a la tracción of 119 MPa | ISO 527 | break, 5 mm/min |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 20 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 20 kJ/m² | ISO 179/2C | 23°C |
Resistencia al choque, ensayo Charpy no entallado | 23.0 °C | 57 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 57 kJ/m² | ISO 179/2C | 23°C |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 196 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 196 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.9E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.9E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 6.4E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 6.4E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Heat deflection temperature, 0.45 MPa | 128 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 128 °C | ASTM D 648 | 3.2 mm, unannealed | |||
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |||
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |||
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |||
Temperatura de flexión bajo carga | 128 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 128 °C | ||||
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101133363- - <br> UL Recognized, 94HB Flame Class Rating: ≥1mm UL 94 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.1 % Show Supplier Material materials with Contracción of 0.1 % | SABIC method | 3.2 mm |
Contracción transversal | 23.0 °C | 0.2 % Show Supplier Material materials with Contracción transversal of 0.2 % | SABIC method | 3.2 mm |
Velocidad de flujo del volumen derretido | 37 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 37 cm³/10min | ISO 1133 | MVR at 300°C/5.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Smart/ID Card, Personal Computing, Wireless Communications, Wearables, Vacuum Cleaner, Lawn/Garden, Enclosures, Electronics, Data Transfer, Audio, Circuit Protection | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 90 to 110.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |