Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.01 % Show Supplier Material materials with Absorción de agua of 0.01 % | ASTM D 570 | (23°C/24hrs) |
Densidad | 23.0 °C | 1.22 g/cm³ Show Supplier Material materials with Densidad of 1.22 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.01 % Show Supplier Material materials with Moisture absorption of 0.01 % | ASTM D 570 | (23°C/50% RH/24 hrs) |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 75 % Show Supplier Material materials with Elongación of 75 % | ASTM D 638 | brk, Type I, 50 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 550 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 550 J/m | ASTM D 256 | notched, 23°C |
Módulo de flexión | 23.0 °C | 2.2 GPa Show Supplier Material materials with Módulo de flexión of 2.2 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Módulo elástico | 23.0 °C | 2.4 GPa Show Supplier Material materials with Módulo elástico of 2.4 GPa | ASTM D 638 | 50 mm/min |
Resistencia a la flexión | 23.0 °C | 79 MPa Show Supplier Material materials with Resistencia a la flexión of 79 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Resistencia a la tracción | 23.0 °C | 46 MPa Show Supplier Material materials with Resistencia a la tracción of 46 MPa | ASTM D 638 | brk, Type I, 50 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 550 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 550 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 7.1E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7.1E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 7.6E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 7.6E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Heat deflection temperature, 1.80 MPa | 106 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 106 °C | ASTM D 648 | 3.2mm, unannealed | |||
Relative temperature index, electrical | 60 °C Show Supplier Material materials with Relative temperature index, electrical of 60 °C | UL 746B | |||
Relative temperature index, mechanical impact | 60 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 60 °C | UL 746B | |||
Relative temperature index, mechanical strength | 60 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 60 °C | UL 746B | |||
Temperatura de flexión bajo carga | 106 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 106 °C | ||||
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100974177- - <br> UL Recognized, 94HB Flame Class Rating: ≥0.6mm UL 94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 1GHz | 23.0 °C | 2.94 [-] Show Supplier Material materials with Dielectric constant, 1GHz of 2.94 [-] | IEC 60250 |
Dissipation factor, 1GHz | 23.0 °C | 5.7E-3 [-] Show Supplier Material materials with Dissipation factor, 1GHz of 5.7E-3 [-] | IEC 60250 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.6 % Show Supplier Material materials with Contracción of 0.6 % | ASTM D 955 | 24 hrs |
Contracción transversal | 23.0 °C | 0.6 % Show Supplier Material materials with Contracción transversal of 0.6 % | ASTM D 955 | 24 hrs |
Velocidad de flujo del volumen derretido | 14 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 14 cm³/10min | ISO 1133 | MVR at 260°C/5.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Data Transfer, Enclosures, Electronic Components, Wireless Communications, Vacuum Cleaner | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 85 to 95.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |