General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad relativa | 23.0 °C | 1.2 [-] Show Supplier Material materials with Densidad relativa of 1.2 [-] | ASTM D 792 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 220 % Show Supplier Material materials with Elongación of 220 % | SABIC - Japan Method | break |
Impact strength, Izod notched, ASTM | 23.0 °C | 833 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 833 J/m | ASTM D 256 |
Módulo de flexión | 23.0 °C | 2.2 GPa Show Supplier Material materials with Módulo de flexión of 2.2 GPa | ASTM D 790 |
Resistencia a la flexión | 23.0 °C | 86 MPa Show Supplier Material materials with Resistencia a la flexión of 86 MPa | ASTM D 790 |
Resistencia a la tracción | 23.0 °C | 65 MPa Show Supplier Material materials with Resistencia a la tracción of 65 MPa | SABIC - Japan Method | yield |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 833 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 833 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 7E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7E-5 1/K | TMA | -30°C to 30°C | ||
Heat deflection temperature, 0.45 MPa | 130 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 130 °C | ASTM D 648 | 3.2 mm, unannealed | |||
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |||
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |||
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |||
Temperatura de flexión bajo carga | 130 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 130 °C | ||||
Inflamabilidad | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=236898- - <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.75mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.75mm UL 94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 60Hz | 23.0 °C | 3.2 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 3.2 [-] | ASTM D 150 | 50/60 Hz |
Sheet resistivity, ROA | 23.0 °C | 1.00E+12 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+12 Ω | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 % Show Supplier Material materials with Contracción of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Personal Computing, Document Handling, Data Transfer, Data Management, Electronic Components | |
Availability | Europe,Asia,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |