LNP™ STAT-KON™ Compound DX09315C

Want to keep this datasheet? Save it now in your required format

Description

LNP STAT-KON DX09315C is carbon fiber filled polycarbonate composite with good flow ability, and high level of cleanliness for the most demanding application. A unique feature of this material is its low C18-C40 hydrocarbons. This compound is manufactured using LNP CCS Technology.

Los datos sobre este material han sido proporcionados por Sabic.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

Propiedades

General

PropertyTemperatureValueComment

Densidad relativa

23.0 °C

1.25 [-]

Show Supplier Material materials with Densidad relativa of 1.25 [-]

ASTM D 792

Mecánica

PropertyTemperatureValueComment

Elongación

23.0 °C

3 %

Show Supplier Material materials with Elongación of 3 %

ASTM D 638 | brk, Type I, 5 mm/min

Impact strength, Izod notched, ASTM

23.0 °C

94 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 94 J/m

ASTM D 256 | notched, 23°C

Impact strength, Izod unnotched, ASTM

23.0 °C

732 J/m

Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 732 J/m

ASTM D 4812 | 23°C

Módulo de flexión

23.0 °C

8.1 GPa

Show Supplier Material materials with Módulo de flexión of 8.1 GPa

ASTM D 790

Módulo elástico

23.0 °C

9.8 GPa

Show Supplier Material materials with Módulo elástico of 9.8 GPa

ASTM D 638 | 5 mm/min

Resistencia a la flexión

23.0 °C

201 MPa

Show Supplier Material materials with Resistencia a la flexión of 201 MPa

ASTM D 790

Resistencia a la tracción

23.0 °C

123 MPa

Show Supplier Material materials with Resistencia a la tracción of 123 MPa

ASTM D 638 | brk, Type I, 5 mm/min

Resistencia al choque, ensayo Izod entallado

23.0 °C

94 kJ/m²

Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 94 kJ/m²

ASTM D 256 | notched, 23°C

Aplicaciones térmicas

PropertyTemperatureValueComment

Coeficiente de dilatación térmica

23.0 °C

1.3E-5 1/K

Show Supplier Material materials with Coeficiente de dilatación térmica of 1.3E-5 1/K

ASTM E 831 | -40°C to 40°C

Coeficiente de dilatación térmica transversal

23.0 °C

7E-5 1/K

Show Supplier Material materials with Coeficiente de dilatación térmica transversal of 7E-5 1/K

ASTM E 831 | -40°C to 40°C

Heat deflection temperature, 1.80 MPa

125 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 125 °C

ASTM D 648 | 3.2mm, unannealed

Relative temperature index, electrical

80 °C

Show Supplier Material materials with Relative temperature index, electrical of 80 °C

UL 746B

Relative temperature index, mechanical impact

80 °C

Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C

UL 746B

Relative temperature index, mechanical strength

80 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C

UL 746B

Temperatura de flexión bajo carga

125 °C

Show Supplier Material materials with Temperatura de flexión bajo carga of 125 °C

Inflamabilidad

UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101901972- - <br> UL Recognized, 94HB Flame Class Rating: ≥1mm UL 94

Eléctrico

PropertyTemperatureValueComment

Sheet resistivity, ROA

23.0 °C

10000 - 500000 Ω

Show Supplier Material materials with Sheet resistivity, ROA of 10000 - 500000 Ω

ASTM D 257

Rheological Properties

PropertyTemperatureValueComment

Contracción

23.0 °C

0.1 %

Show Supplier Material materials with Contracción of 0.1 %

SABIC method | 3.2 mm

Contracción transversal

23.0 °C

0.3 %

Show Supplier Material materials with Contracción transversal of 0.3 %

SABIC method | 3.2 mm

Velocidad de flujo del volumen derretido

26 cm³/10min

Show Supplier Material materials with Velocidad de flujo del volumen derretido of 26 cm³/10min

ISO 1133 | MVR at 300°C/2.16 kg

Technological properties

Property
Application areas

Wireless Communications, Data Management, Document Handling, FPD Handling

Availability

Europe,Asia,Americas

Processing methods

Drying Temperature: 90 to 110.0°C
Drying Time: 3 to 5.0hrs
Melt Temperature: 280 to 320.0°C
Nozzle Temperature: 280 to 320.0°C
Front - Zone 3 Temperature: 280 to 320.0°C
Middle - Zone 2 Temperature: 280 to 320.0°C
Rear - Zone 1 Temperature: 250 to 280.0°C
Mold Temperature: 90 to 120.0°C
Back Pressure: 1 to 5.0MPa
Screw Speed: 30 to 100.0rpm

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.